Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 86.0 µm/m-°C | 47.8 µin/in-°F | ASTM D696 |
PolyOne Geon™ HTX Ultra LA425 Polyvinyl Chloride Alloy (PVC Alloy) Optimum for Black and Darker Colors below 50L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Ductile/Brittle transition as measured by Instrumented Impact is 5 de.. |
|||
CTE, linear, Parallel to Flow | 86.0 µm/m-°C | 47.8 µin/in-°F | ASTM D696 |
PolyOne Geon™ HTX Ultra LA426 Black 2880 Polyvinyl Chloride Alloy (PVC Alloy) Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA426 Black 2880.Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 86.0 µm/m-°C | 47.8 µin/in-°F | ASTM D696 |
PolyOne Edgetek® 5209 Black 30 A 1 Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
CTE, linear, Parallel to Flow | 86.0 µm/m-°C | 47.8 µin/in-°F | ASTM D696 |
PolyOne Edgetek® 5209 Natural 1 Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
CTE, linear, Parallel to Flow | 86.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
47.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp WBG16 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WBG16 is a compound based on Polybutylene Terephalate resin containing Glass Bead, Graphite.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 86.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
47.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP KFB41 (Europe-Africa-Middle East) LNP* THERMOCOMP* KFB41 is a compound based on Acetal Copolymer resin containing Glass Fiber, Glass Bead. |
|||
CTE, linear, Parallel to Flow | 86.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
47.8 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® XD549S PBT+PC (Europe-Africa-Middle East) Xenoy XD549S is an automotive grade, designed for thin wall (2.5 mm.) direct gated exterior parts. The material has an excellent flow. Xenoy XD549S can be painted with primerless solvent or waterbas.. |