Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 84.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
47.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® FR15 ABS Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
47.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® FR15 ABS (Asia Pacific) Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
47.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® FR30U ABS Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
47.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® FR30U ABS (Asia Pacific) Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C | 47.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® ABS 03007 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: ESD ProtectionInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C | 47.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® ABS 03008 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: ESD ProtectionInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C | 47.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® ABS 03009 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Conductive, Electromagnetic Shielding (EMI) and Radio Frequency Shielding (RFI)Information provided.. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C | 47.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® ABS 03010 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: ESD Protection and Good MoldabilityInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C | 47.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® ABS SS5 5% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 5% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C | 47.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® ABS SS5 FR 5% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 5% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation provided by TP Compo.. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C | 47.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® HDPE 04001 LE BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ESD Protection and ConductiveAppearance: BlackProcessing Method: ExtrusionInformation provided by .. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C | 47.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® HTN 05007 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, High Heat Resistance and LubricatedAppearance: BlackInformation provided by TP Composites, .. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C | 47.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6 TL10 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (10%)Features: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C | 47.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6 TL15 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C | 47.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6 TL25 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (25%)Features: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C | 47.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6 TS15 BK Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Silicone Lubricant and PTFE LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composite.. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C | 47.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6 TS18 Nylon 6 Availability: North AmericaForms: PelletsAdditive: PTFE+ Silicone Lubricant(18%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C | 47.0 µin/in-°F | ASTM D696 |
Techmer ES Statiblend® ABS LE Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Low Extractables and Semi ConductiveInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C | 47.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® ABS 03011 BK MB Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Conductive, Electromagnetic Shielding (EMI) and Radio Frequency Shielding (RFI)Appearance: BlackIn.. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C | 47.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® ABS SS15 BK MB 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation provided by TP Composi.. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C | 47.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® ABS SS7 BK MB 7% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 7% Filler by WeightFeatures: ESD ProtectionAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C | 47.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® ABS SS7 MB 7% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 7% Filler by WeightFeatures: ESD ProtectionInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 84.6 µm/m-°C @Temperature 20.0 °C |
47.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PlastxWorld CEVIAN®-V 500 ABS Medium Impact ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |