Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 8.00 µm/m-°C @Temperature 20.0 °C |
4.44 µin/in-°F @Temperature 68.0 °F |
ASTM E381 |
Solvay Specialty Polymers Kadel® E-1230 Polyketone
(discontinued **) Electrical Conductor. High performance proprietary semi-crystalline polymer based resins with exceptional solvent resistance and high temperature performance. They provide strength and stiffness, p.. |
|||
CTE, linear, Parallel to Flow | 8.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
4.44 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP EX03647H PEI LNP LUBRICOMP* EX03647H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 8.00 µm/m-°C @Temperature 23.0 - 60.0 °C |
4.44 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp UCL36AS PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UCL36AS is a compound based on Polyphthalamide resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Heat Stabilized.This data .. |
|||
CTE, linear, Parallel to Flow | 8.00 µm/m-°C @Temperature 23.0 - 60.0 °C |
4.44 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP UCL36ASP PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UCL36ASP is a compound based on Polyphthalamide resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 8.00 µm/m-°C @Temperature 23.0 - 60.0 °C |
4.44 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA6.6 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC006 is a compound based on PA6.6 resin containing Carbon Fiber. Added features include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 8.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
4.44 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP VERTON E9007E PEI LNP* VERTON* E9007E is a compound based on Polyetherimide (PEI) containing 35% Long Carbon Fiber. Added features of this grade include: Structural, High Temperature |
|||
CTE, linear, Parallel to Flow | 8.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
4.44 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON OE006C1 PPS - Linear LNP* STAT-KON* OE006C1 is a compound based on PPS - Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 8.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
4.44 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON RE0069S PA 66 LNP* STAT-KON* RE0069S is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 8.00 µm/m-°C | 4.44 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TW200B6 PA46-CF30 30% Carbon Reinforced, Heat Stabilized, Lubricated |
|||
CTE, linear, Parallel to Flow | 8.00 µm/m-°C @Temperature 150 °C |
4.44 µin/in-°F @Temperature 302 °F |
ASTM E 228 |
DuPont Performance Polymers VESPEL TP-8556 Polyimide Thermoplastic parts from filled PI (polyimide) for balanced mechanical properties and low wear and friction performance in high temperature hostile environmentsInformation provided by DuPont Perform.. |
|||
CTE, linear, Parallel to Flow | 8.00 µm/m-°C @Temperature 55.0 - 160 °C |
4.44 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G45BL BK337 is a 45% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
CTE, linear, Parallel to Flow | 8.00 µm/m-°C | 4.44 µin/in-°F | DIN 53752 |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
CTE, linear, Parallel to Flow | 8.00 µm/m-°C | 4.44 µin/in-°F | DIN 53752 |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
CTE, linear, Parallel to Flow | 8.00 µm/m-°C | 4.44 µin/in-°F | DIN 53752 |
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
CTE, linear, Parallel to Flow | 8.00 - 9.00 µm/m-°C @Temperature 23.0 - 80.0 °C |
4.44 - 5.00 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled PBT Description: Is a PBT, easy-flowing injection-molding grades with 15% glass fibers; for rigid, tough and dimensionally stable technical parts.Applications: Housings, consoles, contact carriers, cove.. |
|||
CTE, linear, Parallel to Flow | 8.00 µm/m-°C | 4.44 µin/in-°F | DIN 53752 |
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
CTE, linear, Parallel to Flow | 8.00 µm/m-°C | 4.44 µin/in-°F | DIN 53752 |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
CTE, linear, Parallel to Flow | 8.00 µm/m-°C | 4.44 µin/in-°F | DIN 53752 |
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |