Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® FR23 ABS Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® FR23 ABS (Asia Pacific) Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® Z48 ABS Automotive. Very high heat resistance with medium impact and good strength properties.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6/6 GF13 IM HS BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6/6 GF14 IM HS L 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6/6 GF14 IM L 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedUL File Nu.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6/6 GF15 IM HS L 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6/6 GF30 IM HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6/6 GF30 IM2 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6/6 GF4 IM L LE Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant, Low Extractables and Impact ModifiedAppearance: Natural ColorInformation provided by TP Composite.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6/6 HI BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedUl File Number: E157318Appearance: BlackProce.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6/6 IM L N Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedUL File Number: E157318Processing Method: Inj.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PA6/6 05012 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 3706 PBT+PC Impact modified PBT+PC resin. Outdoor enclosure. Not available in all colors. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA4/6 GF50 ML2 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Molybdenum Disulfide LubricantFeatures: LubricatedAppearance: BlackUL File Num.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/12 05007 Nylon 612 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PA6/10 BK Nylon 610 Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PA6/6 GF40 IM HS L BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6/6 GF33 IM HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6/6 GF33 IM HS L BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6/6 GF33 IM HS L BKN 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6/6 GF43 IM HS L 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6/6 IM 3757 HS L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Fast Molding Cycle, High Flow, Heat Stabilized, Lubricant and Impact ModifiedProcessing Met.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6/6 IM 408 HS L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6/6 IM HS L BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6/6 IM X Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6/66 IM3 BK Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Copolymer, Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection Moldi.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PA6/6 03002 A MB Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement/Unspecified Filler/Reinfor.Additive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Elec.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C | 44.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PA6/6 05002 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics PREVEX W20 PPE+PS Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F. |