Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 77.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG37CR ABS High performance, injection molding ABS. Overall balance of physical properties, good processability and chemical resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG37CR ABS (Asia Pacific) High performance, injection molding ABS. Overall balance of physical properties, good processability and chemical resistance.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY R2000 PA 66 LNP* LUBRILOY* R2000 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY R2000 PA 66 (Asia Pacific) LNP* Lubriloy* R2000 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY R2000 PA 66 (Europe-Africa-Middle East) LNP* Lubriloy* R2000 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C | 43.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 E4 A1 Nylon 66 Availability: North AmericaForms: PelletsFeatures: High ViscosityInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C | 43.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 E4 HS MB Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Heat Stabilized and High ViscosityInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C | 43.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 E4 IM Nylon 66 Availability: North AmericaForms: PelletsFeatures: Good Toughness and High ViscosityInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C | 43.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 HS N MB Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant, Nucleating Agent and Heat StabilizerFeatures: Lubricated, Fast Molding Cycle, Nucleated and Heat StabilizedTPCI# 8384101Information prov.. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C | 43.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 NAT Availability: North AmericaForms: PelletsAppearance: Natural ColorTPCI# 8384101Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C | 43.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/6 LX Nylon 66 Availability: North AmericaForms: PelletsFeatures: Good Wear Resistance and Low FrictionInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C | 43.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/6 X Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant Features: Lubricated, Good Wear Resistance and Low FrictionInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C | 43.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PA6/6 HS L N Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and Nucleating AgentFeatures: Heat Stabilized, Impact Modified and NucleatedProcessing Method: Injection MoldingIn.. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C | 43.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PA6/6 HS L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Low Viscosity and LubricatedProcessing Method: Injection MoldingInformation provided by TP .. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C | 43.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PA6/6 L UV BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: UV Stabilizer and LubricantFeatures: LubricatedAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C | 43.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PA6/6 M L Nylon 66 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Fast Molding Cycle, Low Viscosity and LubricatedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C | 43.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PA6/6 Nylon 66 Availability: North AmericaForms: PelletsFeatures: Low ViscosityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL N750 PPE+PS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical, TV and Business Equipment applications. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl N750T PPE+HIPS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical, TV and Business equipment applications.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL N850 PPE+PS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL N850 PPE+PS (Asia Pacific) ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C | 43.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 HS MB Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedTPCI# 9094101Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C | 43.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 L N MB Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle and Nucleated TPCI# 8384101Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C @Temperature 20.0 °C |
43.0 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Styron Magnum™ 358HP ABS, High Heat MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
CTE, linear, Parallel to Flow | 77.4 µm/m-°C @Temperature 20.0 °C |
43.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PlastxWorld CEVIAN®-V 450 ABS Heat Resistant ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |