Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 77.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS LNP* Faradex* NS0039 is a compound based on PC/ABS resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Flame Reta.. |
|||
CTE, linear, Parallel to Flow | 77.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS (Asia Pacific) LNP* Faradex* NS0039 is a compound based on PC/ABS resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Flame Reta.. |
|||
CTE, linear, Parallel to Flow | 77.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS (Europe-Africa-Middle East) LNP* Faradex* NS0039 is a compound based on PC/ABS resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Flame Reta.. |
|||
CTE, linear, Parallel to Flow | 77.0 µm/m-°C @Temperature 20.0 °C |
42.8 µin/in-°F @Temperature 68.0 °F |
|
Eastman Eastapak 7352 PET
(discontinued **) Unreinforced Low IV. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003. |
|||
CTE, linear, Parallel to Flow | 77.0 µm/m-°C @Temperature 20.0 °C |
42.8 µin/in-°F @Temperature 68.0 °F |
ISO data |
Dow Isoplast® 151 Polyurethane (PUR-RT), Impact Modified
(discontinued **) ISOPLAST® 151 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include excellent chemical resistance, high heat, low mois.. |
|||
CTE, linear, Parallel to Flow | 77.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
42.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP DL003EXJ PC LNP* Lubricomp* DL003EXJ is a compound based on Polycarbonate containing 15% PTFE. Characteristics of this grade are Easy Molding, Low Extractable, Internally Lubricated, Healthcare. |
|||
CTE, linear, Parallel to Flow | 77.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
42.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP ZX07421 PPO LN:* LUBRICOMP* ZX07421 is a compound based on PPO resin containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 77.0 µm/m-°C @Temperature -40.0 - 100 °C |
42.8 µin/in-°F @Temperature -40.0 - 212 °F |
ASTM E831 |
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by.. |
|||
CTE, linear, Parallel to Flow | 77.0 µm/m-°C @Temperature -40.0 - 100 °C |
42.8 µin/in-°F @Temperature -40.0 - 212 °F |
ASTM E831 |
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided .. |
|||
CTE, linear, Parallel to Flow | 77.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL N190X PPE+HIPS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. Dielectric strength. Suitable for E/E market applications. |
|||
CTE, linear, Parallel to Flow | 77.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL N190X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. RTI Elec/Imp/Str 95/80/95. Dielectric strength. Suitable for E/E market applications. |
|||
CTE, linear, Parallel to Flow | 77.0 µm/m-°C @Temperature 20.0 °C |
42.8 µin/in-°F @Temperature 68.0 °F |
|
Eastman Eastar 6763 PETG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |