Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 57.6 µm/m-°C @Temperature 20.0 °C |
32.0 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Dow Isoplast® 2532 Polyurethane (PUR-RT), Clear Amorphous Polymer
(discontinued **) ISOPLAST® 2532 resin is a clear amorphous polymer with the chemical resistance of crystalline resins specially designed for medical applications. Its outstanding properties include clarity, excelle.. |
|||
CTE, linear, Parallel to Flow | 57.6 µm/m-°C @Temperature 20.0 °C |
32.0 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Dow Isoplast® 302 Polyurethane (PUR-RT), Clear Amorphous Polymer
(discontinued **) ISOPLAST® 302 resin is a clear amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include clarity, excellent chemical resistance, toughness and high he.. |
|||
CTE, linear, Parallel to Flow | 57.6 µm/m-°C | 32.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PC SS10 10% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: ConductiveInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 57.6 µm/m-°C | 32.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 GF13 FR BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 13% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedAppear.. |
|||
CTE, linear, Parallel to Flow | 57.6 µm/m-°C | 32.0 µin/in-°F | ASTM D696 |
Techmer ES Statiblend® PC FR BK Availability: North AmericaForms: PelletsAntistaticFeatures: Flame Retardant and Semi ConductiveUL File Number: E157318Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 57.6 µm/m-°C @Temperature 20.0 °C |
32.0 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Styron Pulse® 759 ABS + Polycarbonate, 15% Glass Reinforced PULSE® 759 Engineering resin is a 15% glass reinforced resin designed to provide excellent processability, high heat resistance, and practical toughness. PULSE 759 Engineering resin has been used.. |
|||
CTE, linear, Parallel to Flow | 57.6 µm/m-°C @Temperature 20.0 °C |
32.0 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Styron Pulse® 959 ABS + Polycarbonate, 10% Glass Reinforced PULSE® 959 Engineering resin is a 10% glass reinforced resin designed to provide excellent processability, high heat resistance, and practical toughness. PULSE 959 Engineering resin has been used.. |
|||
CTE, linear, Parallel to Flow | 57.6 µm/m-°C | 32.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PA6 GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight/Unspecified Filler/Reinfor.Additive: LubricantFeatures: Conductive and LubricatedAppear.. |
|||
CTE, linear, Parallel to Flow | 57.6 µm/m-°C | 32.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA4/6 GF5 IM HS BK 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact Modifie.. |
|||
CTE, linear, Parallel to Flow | 57.6 µm/m-°C | 32.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 GF10 FR BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightFeatures: Flame Retardant Appearance: BlackProcessing Method: Injection MoldingInformation provided by.. |
|||
CTE, linear, Parallel to Flow | 57.6 µm/m-°C | 32.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 GF15 FR BK 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedAppear.. |
|||
CTE, linear, Parallel to Flow | 57.6 µm/m-°C | 32.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PC SS15 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |