Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 5.00 µm/m-°C | 2.78 µin/in-°F | Below Tg; ISO 11359 |
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c.. |
|||
CTE, linear, Parallel to Flow | 5.00 µm/m-°C @Temperature 23.0 - 60.0 °C |
2.78 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RCL36 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RCL36 is a compound based on PA 66 resin containing PTFE, Carbon Fiber. Added features include: Electrically Conductive, Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 5.00 µm/m-°C @Temperature -50.0 - 50.0 °C |
2.78 µin/in-°F @Temperature -58.0 - 122 °F |
1 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621.. |
|||
CTE, linear, Parallel to Flow | 5.00 µm/m-°C @Temperature 23.0 - 60.0 °C |
2.78 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON OE008 PPS (Europe-Africa-Middle East) LNP * Stat-kon* OE 008 is a compound based on PPS-Linear resin containing Carbon Fiber. Added features include: Electically Conductive. |
|||
CTE, linear, Parallel to Flow | 5.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
2.78 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP JF008E PES LNP* THERMOCOMP* JF008E is a compound based on Polyethersulfone containing 40% Glass Fiber. Characteristics of this grade are: Easy Molding. |
|||
CTE, linear, Parallel to Flow | 5.00 µm/m-°C @Temperature -40.0 - 150 °C |
2.78 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP LC006EXQ PEEK LNP* THERMOCOMP* LC006EXQ is a compound based on Polyetheretherketone containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding. |
|||
CTE, linear, Parallel to Flow | 5.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
2.78 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP WF002 PBT LNP* THERMOCOMP* WF002 is a compound based on PBT containing 10% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 5.00 µm/m-°C | 2.78 µin/in-°F | TMA |
Vyncolit A2990 Glass Fiber Reinforced Novolac Phenolic Resole resin based, glass fiber reinforced. Good mechanical properties, combined with superior electrical insulation properties. Among others used for commutator applicationsInformation provided by .. |
|||
CTE, linear, Parallel to Flow | 5.00 - 20.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
2.78 - 11.1 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Dry) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
CTE, linear, Parallel to Flow | 5.00 µm/m-°C @Temperature -50.0 - 50.0 °C |
2.78 µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr.. |
|||
CTE, linear, Parallel to Flow | 5.00 - 10.0 µm/m-°C @Temperature 50.0 - 100 °C |
2.78 - 5.56 µin/in-°F @Temperature 122 - 212 °F |
ISO 11359-2 |
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc.. |
|||
CTE, linear, Parallel to Flow | 5.00 µm/m-°C @Temperature 23.0 - 80.0 °C |
2.78 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
BASF Ultradur® S 4090 GM13 5/15% Glass/Mineral Filled PBT Description: Is a PBT + ASA, injection-molding grades reinforced with 5% glass fiber and 15% mineral, for laminar parts with high demands on dimensional stability and low warpage, e.g. lids, ventila.. |
|||
CTE, linear, Parallel to Flow | 5.00 µm/m-°C @Temperature -30.0 - 100 °C |
2.78 µin/in-°F @Temperature -22.0 - 212 °F |
ISO 11359-2 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3230A PP SABIC® PPcompound G3230A is a general purpose, 30% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS ID is 109612410 |