Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 GF30 FR NAT 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedAppear.. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® ABS E GM15 LE 15% Glass Filled Availability: North AmericaFeatures: Low ExtractablesForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® ABS E GM5 LE 5% Glass Filled Availability: North AmericaFeatures: Low ExtractablesForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® ABS WM20 20% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® ASA GF15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceInformation provided by TP Composites.. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® HTN GF HS L High Temp Nylon 50% Glass Filled Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Heat ResistanceInformation provided by TP Composit.. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF/B20 A2 20% Glass Fiber/Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Glass Bead, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformation .. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF/B20 A3 BK 20% Glass Fiber/Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Glass Bead, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: .. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PBT GF20 BK007 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackTPCI# 6225111Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP 0096 S2 LE Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP 0096 S3 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP 0112 B AM2 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforAdditive: Antimicrobial (Fungicide)Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP 0159 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP 0254 S Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP 0320 S1 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Good Corrosion ResistanceInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP GF20 CC LE 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Chemically Coupled and Low ExtractablesInformation provided by TP Composites, .. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PA6 SF76 L Availability: North AmericaForms: Pellets Additive: Lubricant and Strontium Ferrite (76%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES Statiblend® ABS GF20 AS 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 GF33 FR HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform.. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® ABS IM TM20 20% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation p.. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® HDPE LGF50 12 mm 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® LDPE 0098 S LE Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforAdditive: Heat StabilizerFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® TPX-HTN-01040 A 45% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 45% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthInformat.. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® ABS GF15 A1 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc. |