Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Ravago Manufacturing Americas Hylon® N1213HL BK Nylon 6/6 Available in North America Filler: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantForm: Pellets Proces.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
15.0 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® A 218 V25 NAT BA PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, specially stabilized to improve its resistance to oils and greases, for injection molding.Available in: Asia PacificProduct Application.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
15.0 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® A 218 V25 Natural B PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, specially stabilized to improve its resistance to oils and greases, for injection molding.Available in: EuropeProduct Applications: Thi.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
15.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA6.10 (Europe-Africa-Middle East) LNP*Lubricomp* QFL36 is a compound based on PA 6/10 resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® TPX-HTN-01031 35% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 35% Filler by WeightAdditive: Heat Stabilizer Features: Flame Retardant, Heat Stabilized and High Temperature Strength UL .. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PET GF/M35 35% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 35% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP E GF40 CC 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Chemically Coupled, Heat Stabilized and High Viscosit.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP GF40 CC 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6 GF15 TL15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: Heat Stabilized and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Heat Stab.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6 GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: Heat Stabilized and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Heat Stab.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/6 CF30 TL12 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE + Silicone Lubricant(15%)Features: Lubricated and Good Wear ResistanceTPCI# 6466101Inf.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/6 GF30 IM TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resi.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/6 TL20 HS L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant(20%)Features: Lubricated, Heat Stabilized and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/6 TS20 HS Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilized, PTFE Lubricant(18%) and Silicone Lubricant (2%)Features: Lubricated, Good Wear Resistance and Heat StabilizedInformation provide.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PPA CF30 TL15 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, High Heat Resistance and Low.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
15.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK3020 PC LNP* Thermocomp* Lexan_LGK3020 compound is a glass reinforced. Flame retardant. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
15.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermotuf PF007IX2 PA 6 (Europe-Africa-Middle East) LNP * THERMOTUF* PF007IX2 is a compound based on PA 6 resin containing Glass Fiber. Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
15.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AG6ST01 PA66, Glass Fiber Reinforced, Impact Modified, Injection Molding Staramide AG6ST01 is an Impact Modified, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
15.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BG6ST01 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG6ST01 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 3412R PC 20% GR, provides improved mechanical properties and UL94 V-1 rated at 0.058"". Internal mold release added. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM E831 |
Sumitomo Bakelite North America Epiall® 1908M-1 Short Glass Fiber Reinforced Epoxy Epiall 1908M-1 is a short glass fiber reinforced epoxy molding compound with excellent dimensional stability, good strength properties, and good electrical insulation properties.Information provided.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PBT GF30 FR-S 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame Retardant and Non-BloomingProcessing Method: Injection MoldingInformation provided by .. |