Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 3413R PC (Europe-Africa-Middle East) LEXAN 3413R is a high viscosity, 30% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP AFP26 ABS (Europe-Africa-Middle East) LNP* Lubricomp* AFP26 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, PTFE, Silicone. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
13.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP DFL14 PC LNP LUBRICOMP* DFL14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 150 °C |
13.9 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2210R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | |
Solvay Specialty Polymers Veradel® 3320GF Polyethersulfone (PESU), 20% Glass Fiber Veradel® 3320GF is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® V9260CS PET (Asia Pacific) Color Stable Glass filled PET |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® V9260CS PET (Europe-Africa-Middle East) Color Stable Glass filled PET |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
13.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Stat-kon NX03602 PC+ABS LNP STAT-KON* NX03602 is a compound based on PC+ABS Blend resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supplied by .. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
Styrolution Luran® 378 P G7 35% Glass Filled SAN Description: Glass-reinforced grade with very high stiffness and low thermal coefficient of liner expansion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP QF0069 PA6.10 (Europe-Africa-Middle East) LNP* THERMOCOMP* QF0069 is a compound based on PA610 resin contaning Glass Fiber, Flame Retardant. Added features include: Flame retardant. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp RF006XXP PA 66 (Europe-Africa-Middle East) 30% glass fibre reinforced Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 20.0 °C |
13.9 µin/in-°F @Temperature 68.0 °F |
ASTM E-831 |
Sumitomo Bakelite North America E 8353-706R-1 Hardware Grade Epoxy Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp PF006 PA 6 (Europe-Africa-Middle East) 30% glass fibre reinforced Polyamide 6 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 20.0 °C |
13.9 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit X689 Novolac Phenolic Glass fiber filled and molybdeendisulfide modified phenolic molding compound with excellent mechanical and thermal properties and lower thermal expansion coefficient. It has excellent friction prop.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® 2SV-30H nat PA610-GF30 Product Description: GRILAMID XE3976 natural 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mat.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® AG-30 H PA66 Product description: Grilon AG-30 H black 9836 is a normal viscosity, specially heat stabilized PA 66 injection molding grade with 30% glass fibres. Grilon AG-30 H black 9836 has the following impor.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BG-25 S PA6-GF25 Product description: Grilon BG-25 S is a heat stabilized PA6 injection molding grade with 25 % glass fibers. Grilon BG-25 S has the following important properties: Excellent surface finishEasy flowi.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® 46HF4530 PA46-GF30 30% Glass Reinforced, Heat Stabilized, High Flow, for E&E applications |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TC153 PA46 FR(17) Thermal conductive material, Flame Retardant, Heat Stabilized |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TE200F8 PA46-GF40 40% Glass Reinforced, Heat Stabilized, for E&E applications |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TW241B3 PA46-CF15 15% Carbon Reinforced, Heat Stabilized, Lubricated |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TW242FM10 PA46-(GF+MF)50 50% Glass/Mineral Reinforced, Heat Stabilized |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® 940 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 40% Glass/Mineral Reinforced Polyethylene TerephthalateInformation provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AG6H PA66, 30% Glass Filled, Injection Molded AG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® AV2 370 HF PET-GF35 35% Glass Reinforced, Brake Booster Body Valves, High Flow |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® VX4029 PBT (Europe-Africa-Middle East) VALOX VX4029 is a 30% glass reinforced PBT injection moulding resin with excellent strength, stiffness, dimensional stability and high heat resistance. This grade is a 420 with reduced additive load.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TS200B3 PA46-CF15 15% Carbon Reinforced |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TS200F6 PA46-GF30 30% Glass Reinforced |