Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 177 µm/m-°C @Temperature 20.0 °C |
98.3 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Kynar® FLEX 2750 PVDF