Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 16.2 µm/m-°C @Temperature -20.0 - 150 °C |
9.00 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2310 PEI 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C @Temperature -20.0 - 150 °C |
9.00 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2310 PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C @Temperature -20.0 - 150 °C |
9.00 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2310R PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 G/C40 L UV 40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Good UV Resistance and LubricatedTPCI# 6024102Informa.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF30 HF L BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant Features: Lubricated and High FlowAppearance: BlackInformation provi.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF30 HS BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF30 L UV 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF30 RM BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Low Moisture AbsorptionAppearance: BlackTPCI# 9719102Information provided by T.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF33 L BK001 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: BlackTPCI# 8221102Information provid.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF33 L NAT004 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: Natural ColorTPCI# 9411102Informatio.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF40 L 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant Features: LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF40 RM HS BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat Stabilizer Features: Heat Stabilized and Low Moisture AbsorptionAppearanc.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF43 L BK 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackProcessing Method: Injection Mol.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF/M40 B1 BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearan.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF/M40 HS L NAT 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF/M40 HS Up BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat Sta.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF50 HS L BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF50 L BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF50 L UV 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformat.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PPS 0231 B LE Availability: North AmericaForms: PelletsFeatures: High Density and Low ExtractablesAppearance: OpaqueInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® R60 G33-L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: Natural ColorTPCI# 9208102Information.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PA6 GF30 RM BK Nylon 6 Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES Statiblend® PA12 CB Availability: North AmericaForms: PelletsAdditive: Carbon BlackFeatures: ConductiveAppearance: BlackTPCI# 9872105Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PBT G/CF30 IM 15% Glass/Carbon Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 15% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: Natural ColorInform.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PPS 0237 A Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PPS 0334 A Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PEI GF30 TL15 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 GF50 FR UV X BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 50% Filler by WeightAdditive: Flame Retardant and UV StabilizerFeatures: Flame RetardantAppearance: BlackProcessing Method.. |