Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 150 µm/m-°C | 83.3 µin/in-°F | Above Tg, Result based on 450G; ISO 11359 |
Victrex® PEEK 600G Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BC 304 H3.0 000000 Nylon 6 PA 6, injection molding grade, non-reinforced, elastomer-modified, extremely high notched impact strength, including in the dry state and at low temperatures, also applicable for barrier layers in e.. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 23.0 - 55.0 °C |
83.3 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® TP 142-011 900116 Nylon 6 PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
1 |
Solvay Specialty Polymers Polidan® T/A-LV Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LV is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
|
Covestro Desmopan® 385 Thermoplastic Polyurethane Desmopan 385 is a TPU on the basis of a standard ester.Applications: Screen sections, films, hoses, seals, technical automotive parts.Information provided by Bayer.As of 1 September 2015, Bayer Mate.. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® EM550 55 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® EM550 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® EM630-H Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® PL381 Injection Molding Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® PL381 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
DSM Arnitel® PL381-H TPC-ET Injection Molding |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® PM381 38 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® PM381 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
DSM Arnitel® VT3104 TPC-ET Extrusion Grade |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
|
Covestro Texin® 285 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Baye.. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® AZ 3/2 PA66 Product description: Grilon AZ 3/2 is an unreinforced and impact modified PA66 injection molding grade. Grilon AZ 3/2 has the following important properties: Excellent toughness at low temperaturesE.. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® EL550 55 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® BESN F15 TL Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11-P,EHL,16-001High flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High burst pressure and impact strength.. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 2248 TC Polypropylene Nucleated grade with antistatic agent for injection moldings.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 2300 L Polypropylene Injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 2309 L Polypropylene Cast film and thermoformed partsData was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 2348 M Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 2348 TC Polypropylene Grade with nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 2500 H Polypropylene Injection molded parts, blow moldings and thermoformed parts.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 2600 M Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 2600 PC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 2700 L Polypropylene UV stabilized grade for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 2800 J Polypropylene Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 2440 K Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 2900 NC Polypropylene Injection molded partsData was collected by ISO methods and provided by BASF. |