Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 148 µm/m-°C @Temperature 20.0 °C |
82.2 µin/in-°F @Temperature 68.0 °F |
|
Eastman Ecdel PCCE 9965 Copolyester Ether Elastomer ISO data as provided by the manufacturer, Eastman Chemical |