Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 20.0 °C |
72.2 µin/in-°F @Temperature 68.0 °F |
|
Eastman Tenite 264-10 CAB Cellulose Acetate Butyrate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 20.0 °C |
72.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
KEP Kepital® F10 Standard Grade/High Viscosity Acetal Homopolymer Extrusion: electrical parts, machine/mechanical parts, industrial parts, automotive parts, applications, electronic data processing parts, thick-walledKepital® is a registered trademark of Korea .. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® DP 2325 H3.0 000000 Nylon 66 PA 66, injection molding grade, non-reinforced, elastomer-modified, good heat-ageing resistance, extremely high notched impact strength even at dry state and at low temperatures |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® B 1100 000000 PBT PBT, non-reinforced, extrusion, injection molding, improved flowability |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 80.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 325 PBT (Europe-Africa-Middle East) VALOX 325 is a general purpose, unreinforced PBT injection moulding resin. Applications: sprinklers and nozzles, pumps, doorhandles, tank covers, pens and pencils. |
|||
CTE, linear, Parallel to Flow | 130 - 150 µm/m-°C @Temperature 0.000 - 40.0 °C |
72.2 - 83.3 µin/in-°F @Temperature 32.0 - 104 °F |
1 |
Solvay Specialty Polymers Solef® 32008 Polyvinylidene Fluoride (PVDF) Solef® 32008 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional .. |
|||
CTE, linear, Parallel to Flow | 130 - 180 µm/m-°C @Temperature 0.000 - 40.0 °C |
72.2 - 100 µin/in-°F @Temperature 32.0 - 104 °F |
1 |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF) Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Features: Copolymer; High ViscosityUses: PipingAdditional Properties: Crystallization Heat - ASTM .. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 80.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® FXV310SK PBT (Europe-Africa-Middle East) LIMITED USE, No New Customers / Applications as of Jan. 2010: VALOX FXV310SK is an unreinforced PBT injection moulding resin with high flow characteristics and containing a metal sparkle Visual FX. .. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 60.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® VX3101N PBT (Europe-Africa-Middle East) VALOX VX3101N is an unreinforced PBT injection moulding resin, with excellent flow properties, good hydrolitical stability and chemical resistance. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 80.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® CL500U PBT+PC (Europe-Africa-Middle East) XENOY CL500U is a semi-crystalline blend, developed for exterior automotive parts ( except bumper shells ) and non automotive parts, requiring good impact, excellent chemical resistance and UV stabi.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature -40.0 - 60.0 °C |
72.2 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl N190A PPE+PS (Asia Pacific) Low heat, flame retardant PPO/HIPS alloy. Internal flammability results only.Not a UL recognised material.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® R 50 H NZ PA6 Product description: Grilon R 50 H NZ is a high viscosity, unreinforced, heat stabilized, impact modified PA6 extrusion blow molding grade. Grilon R 50 H NZ has the following important properties: V.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST811HS BK038 Nylon 6
(Unverified Data**) Zytel® ST811HS BK038 is a flexible, non-plasticized, black Super Tough nylon 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores an.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 25 W 10 H X PA12 Product Description: Grilamid L 25 W 10 HX is a semi flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 10 HX is impact modified and heat and UV stabilized.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Barlog Plastics KEBAFORM C 906 LF POM Copolymer unreinforced, improved wear and friction POMInformation provided by BARLOG plastics GmbH. |
|||
CTE, linear, Parallel to Flow | 130 - 160 µm/m-°C @Temperature 23.0 - 80.0 °C |
72.2 - 88.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultradur® B 4560 PBT Description: Medium viscosity injection molding grade for industrial parts in the automotive field, for example for head lamp bezel. Suitable for direct metalizing.Information provided by BASF |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359 |
BASF Ultraform N 2640 Z4 UNC Q600 POM Ultraform N2640 Z4 UNC Q600 is a high toughness, elastomer-modified injection molding POM grade. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
DIN 53752 |
BASF Ultraform® N2640 E2 POM Description: Is a POM + MBS, elastomer-modified injection-molding grade with enhanced toughness and high weld line strength.Information provided by BASF |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
BASF Ultraform® N2640 Z2 POM + PUR Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
BASF Ultraform® N2650 Z4 POM + PUR Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 20.0 °C |
72.2 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® AMN D Nylon 12, Rigid, Injection Grade (Conditioned) Designation ISO 1874-PA12,MR,14-010Rigid grade for injection molding. Available colors: black, natural, orange, red and white. Possibilities of heat and light stabilizing agents. Mold-release agent... |