Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature 20.0 °C |
7.22 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® S223-PG6U (Dry) 33% Glass Reinforced, Impact Modified Nylon 66 (North America)
(discontinued **)& Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
7.22 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DX09315C PC (Asia Pacific) LNP* Stat-Kon* DX09315C is carbon fiber filled polycarbonate composite with good flow ability, and high level of cleanliness for the most demanding application. A unique feature of this material is .. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
7.22 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DF00A1P PC (Asia Pacific) LNP* Thermocomp* DF00AIP is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High Modulus, low warpage, Non-Brominated & Non.. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C | 7.22 µin/in-°F | ASTM E831 |
Sumitomo Bakelite North America RX® 643 Fiberglass Reinforced Phenolic RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10.Information pro.. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
7.22 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP JCL36E PES LNP* LUBRICOMP* JCL36E is a compound based on Polyethersulfone (PES) resin containing 30% Carbon Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
7.22 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP WCL36 PBT LNP* LUBRICOMP* WCL36 is a compound based on PBT resin containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
7.22 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp OC004 PPS - Linear (Europe-Africa-Middle East) LNP* THERMOCOMP* OC004 is a compound based on PPS-Linear resin containing Carbon Fiber. Added features include : Electrically Conductive.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C | 7.22 µin/in-°F | ASTM E831 |
Sumitomo Bakelite North America XB-22 Fiberglass Reinforced Phenolic Novolac XB-22 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is formulated for low thermal condu.. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C | 7.22 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSG-60/4 W PA666-GF60 Product description: Grilon TSG-60/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
7.22 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starglas OC004 PPS, 20% Carbon Filled, Injection Molded Starglas OC004 is a 20% Carbon Fiber Reinforced PPS Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
7.22 µin/in-°F @Temperature 73.4 - 131 °F |
DIN 53752 |
BASF Ultraform® N2650 Z4 (LEV) POM Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr.. |
|||
CTE, linear, Parallel to Flow | 13.0 - 16.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
7.22 - 8.89 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
BASF Ultradur B 4500 PBT Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
7.22 µin/in-°F @Temperature 73.4 - 131 °F |
DIN 53752 |
BASF Ultraform® N2650 Z2 (LEV) POM Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr.. |
|||
CTE, linear, Parallel to Flow | 13.0 - 16.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
7.22 - 8.89 µin/in-°F @Temperature 73.4 - 176 °F |
|
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |
|||
CTE, linear, Parallel to Flow | 13.0 - 16.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
7.22 - 8.89 µin/in-°F @Temperature 73.4 - 176 °F |
|
BASF Ultradur B 6550 PBT Ultradur B 6550 is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
7.22 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOTUF OF008I PPS - Linear (Europe-Africa-Middle East) LNP* Thermotuf* OF008I is a compound based on PPS - Linear resin containing Glass Fiber. Added features of this material include: High Impact. |