Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 128 µm/m-°C @Temperature 23.0 - 60.0 °C |
71.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP ML008 PP (Europe-Africa-Middle East) LNP* LUBRICOMP* ML008 is a compound based on Polypropylene resin containing PTFE. Added Features include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 128 µm/m-°C @Temperature -30.0 - 30.0 °C |
71.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-LOY M3000C PP LNP* STAT-LOY* M3000C is a compound based on unfilled Polypropylene resin. Added features of this grade include: Clean Compound System, Antistat. |
|||
CTE, linear, Parallel to Flow | 128 µm/m-°C | 71.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® POM CO SL2 MB Acetal Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and CopolymerTPCI# 9809114Information provided by TP Composites, Inc. |