Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 121 µm/m-°C @Temperature 20.0 °C |
67.2 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS Centrex® 813 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
CTE, linear, Parallel to Flow | 121 µm/m-°C @Temperature 23.0 - 60.0 °C |
67.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-LOY M3000 PP (Europe-Africa-Middle East) LNP* Stat-loy* M3000 is a compound based on Polypropylene resin. Added features of this material include: Antistat, High Impact. |
|||
CTE, linear, Parallel to Flow | 121 µm/m-°C @Temperature -40.0 - 40.0 °C |
67.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66 (Asia Pacific) LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder, Impact Modifier. Added features of this material include: Electrically Conductive, High Impact. |
|||
CTE, linear, Parallel to Flow | 121 µm/m-°C @Temperature -30.0 - 30.0 °C |
67.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Thermocomp YF004 Polyester Elastomer LNP THERMOCOMP* YF004 is a compound based on Polyester Elastomer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 121 µm/m-°C @Temperature 20.0 °C |
67.2 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS Centrex® HGM ASA Blend
(discontinued **) Key Features:UnfilledLight stabilized or stable to lightU.V. stabilized or stable to weatherHeat stabilized or stable to heatSuitable processing methods:Injection moldingInformation provided by Baye.. |