Polymer Property : Heat of Fusion = 24.1 BTU/lb Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat of Fusion 56.0 J/g
24.1 BTU/lb
ASTM E793
Eastman 9921 PET Film  (discontinued **)
VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p..
Heat of Fusion 56.0 J/g
24.1 BTU/lb
ASTM E793
Eastman 9921 PET Injection Molded  (discontinued **)
VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p..
Heat of Fusion 56.0 J/g
24.1 BTU/lb
80°C to end of melting
Solvay Specialty Polymers Solef® 1015/0078 PVDF Homopolymer  (discontinued **)
Key features of this grade: Plasticized, Offshore, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorina..
Heat of Fusion 56.0 J/g
24.1 BTU/lb
Crystallization Heat
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer  (discontinued **)
Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c..
Heat of Fusion 56.0 J/g
24.1 BTU/lb
ASTM E793
Eastman 9921W PET Film  (discontinued **)
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters ..
Heat of Fusion 56.0 J/g
24.1 BTU/lb
ASTM E793
Eastman 9921W PET Injection Molded  (discontinued **)
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters ..