Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Fusion | 59.0 J/g | 25.4 BTU/lb | ASTM E793 |
Eastman CB12 PET
(discontinued **) Voridian CB12 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. CB12 delivers fast, efficient processing and good ov.. |
|||
Heat of Fusion | 59.0 J/g | 25.4 BTU/lb | Crystallization Heat |
Solvay Specialty Polymers Solef® 3108/0903 Anti-static PVDF Compound
(discontinued **) Key features of this grade: Anti-static, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crystall.. |
|||
Heat of Fusion | 59.0 J/g | 25.4 BTU/lb | Crystallization Heat |
Solvay Specialty Polymers Solef® 3208/0150 Anti-friction PVDF Compound
(discontinued **) Key features of this grade: Anti-friction, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
Heat of Fusion | 59.0 J/g | 25.4 BTU/lb | Crystallization Heat |
Solvay Specialty Polymers Solef® 8808/0902 Carbon Fiber Reinforced PVDF Compound
(discontinued **) Key features of this grade: Carbon Fiber Reinforcement, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinate.. |
|||
Heat of Fusion | 59.0 J/g | 25.4 BTU/lb | DSC on the first heating cycle; ASTM E793 |
DAK Americas Laser+® MB912 PET Product Description: Laser+® MB912 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. It delivers fast, efficient pr.. |
|||
Heat of Fusion | 59.0 J/g | 25.4 BTU/lb | Crystallization Heat |
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer
(discontinued **) Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Heat of Fusion | 59.0 J/g | 25.4 BTU/lb | ASTM E793 |
Eastman VersaTray 12822 Plastic
(discontinued **) VersaTray plastic 12822 is a polyethylene terephthalate resin designed for use as a base resin for crystallized PET (CPET) food trays and other high temperature food packaging applications. CPET foo.. |