Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Fusion | 32.0 J/g | 13.8 BTU/lb | Crystallization Heat |
Solvay Specialty Polymers Solef® 31008 PVDF Copolymer
(discontinued **) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
Heat of Fusion | 32.0 J/g | 13.8 BTU/lb | ASTM E793 |
Eastman Eastar A150 Copolyester, Film Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan.. |