Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Monmouth Rubber & Plastics Durafoamâ„¢ C41 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Minimum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Monmouth Rubber & Plastics Durafoamâ„¢ C42 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Minimum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Monmouth Rubber & Plastics Durafoamâ„¢ C43 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Minimum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Monmouth Rubber & Plastics Durafoamâ„¢ C44 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Minimum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Monmouth Rubber & Plastics Durafoamâ„¢ C45 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |