Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -14.0 °C | 6.80 °F | Brittleness Temperature |
DuPont Performance Polymers Hypalon® 48 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound
(d Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato.. |
|||
Minimum Service Temperature, Air | -14.0 °C | 6.80 °F | Brittleness Temperature |
DuPont Performance Polymers Hypalon® 48 Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound
(discon Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont .. |
|||
Minimum Service Temperature, Air | -14.0 °C | 6.80 °F | Torsion Stiffness Temperature |
Stir SpA Giesse EPM/86 (PVC) Application: Extrusion medical parts - low flexibilityInformation provided by STIR SpA |
|||
Minimum Service Temperature, Air | -14.0 °C | 6.80 °F | TR test, TR10 |
Daikin DAI-EL G-555 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 69% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Products with excellent balance of.. |
|||
Minimum Service Temperature, Air | -14.0 °C | 6.80 °F | TR test, TR10 |
Daikin DAI-EL G-558 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 69% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Low gasoline permeability and good.. |
|||
Minimum Service Temperature, Air | -14.0 °C | 6.80 °F | TR test, TR10 |
Daikin DAI-EL G-952 Fluoroelastomer Terpolymer, Peroxide Curable Grade, 69% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Good solvent resistance and low-temperature characteristics.Information provided by Daikin Industrie.. |
|||
Minimum Service Temperature, Air | -14.0 °C | 6.80 °F | TR test, TR10 |
Daikin DAI-EL G-551 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 69% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Products with excellent balance of.. |