Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M Bumpon™ SJ6008 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M Bumpon™ SJ6032 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FL028 Indoor UL Recognized Lexan Label Products 3M™ Indoor UL Recognized Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P1.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FM01G Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FM05E Indoor UL Recognized Brite Silver Polyester Label Products 3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FM061 Indoor UL Recognized Brite Silver Polyester Label Products 3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FM07N Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Matte Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester ov.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FM110 Indoor UL Recognized Brushed Silver Polyester Label Products 3M™ Indoor UL Recognized Brushed Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utili.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FM1183 Indoor UL Recognized MC Polyester Label Products 3M™ Indoor UL Recognized MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These po.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Service |
3M FM292 Indoor UL Recognized Clear Polyester Overlaminate Label Products 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FP014 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Service |
3M FP024901 White Polypropylene Label Products 3M™ White Polypropylene Label Products are matte white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a general.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FP032302W White Metallized Polypropylene Label Products 3M™ White Metallized Polypropylene Label Products FP032302, FP032302W and FP032305 are a white opaque material that offers excellent durability and opacity. These label products utilize 3M™ Adhesi.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FP0869 Removable Clear Polypropylene Label Products 3M™ Removable Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ultra removable acrylic designed f.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FP101 Clear Polypropylene Label Product 3M™ Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1410, which is a general purpose permanent tackified acrylic t.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FP532 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FS042 Clear Polystyrene Label Products 3M™ Clear Polystyrene Label Products are hard, rigid film materials that offer economic alternatives for indoor applications. These polystyrene labels utilize 3M™ Adhesive P1212, which is a high c.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FV062 Semi-Rigid White Vinyl Label Product 3M™ Semi-Rigid White Vinyl Label Products are white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clarity general.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FV090 Soft Translucent Vinyl Label Products 3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M Bumpon™ SJ5916 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FA03E Matte Clear Acetate Label Products 3M™ Matte Clear Acetate Label Products offer consistent, high quality film appearance. This film die-cuts easily which helps extend die life in comparison with polyester label stocks. These acetate.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FP012 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FV02800N Textured Vinyl Label Products 3M™ Textured Vinyl Label Products are flexible and conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212 which is a high.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M OFM0403 Outdoor UL Recognized White Polyester Label Product 3M™ Outdoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ .. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M OFM040E Outdoor UL Recognized White Polyester Label Product 3M™ Outdoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ .. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Service |
3M PS190 White Yupo™ TIS Label Products 3M™ White Yupo™ TIS Label Products are white treated polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a g.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FM048 Clear Polyester Label Product 3M™ Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for demanding applications such.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FV038 Indoor UL Recognized White Vinyl Label Products 3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,.. |
|||
Minimum Service Temperature, Air | 5.00 °C | 41.0 °F | Application |
3M FM009 Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |