Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
Chesterton 601 Chain Drive Pin & Bushing Lubricant Description: Chesterton® 601 Chain Drive Pin & Bushing Lubricant is and has been the premium quality light lubricant of choice in industry for over thirty years. This superior lubricant was special.. |
|||
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
Chesterton 622 White Grease Description: Chesterton® 622 White Grease is a pure mineral oil grease with PTFE added designed for applications where a clean, nonstaining, food grade lubricant is required. It is a superior, mult.. |
|||
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | See Note 1. |
ChevronTexaco 904 Grease NLGI Grade 1/2 Texaco 904 Grease is a calcium soap grease. It contains graphite which enhances its lubricity.Typical test data are average values only. Minor variations which do not affect product performance are .. |
|||
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | See Note 1. |
ChevronTexaco Marfak® Heavy Duty 3 Texaco Marfak grease delivers value through:Good film strengthGood rust and corrosion protection, even in wet conditions.Texaco Marfak greases are fibrous sodium soap greases. It resists oil separat.. |
|||
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | See Note 1. |
ChevronTexaco Thermatex® EP NLGI Grade 2 Texaco Thermatex EP greases deliver value through:High temperature stability — Will not melt at high temperatures, but will remain in place on bearing surfaces and continue to provide excellent lub.. |
|||
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
3M 3334 Aluminum Foil/Scrim/PE Facing Tape 3M™ Aluminum Foil Tape 3334 has a high performance aluminum foil/bidirectional fiberglass scrim/polyethylene film laminate backing coated with a special pressure sensitive acrylic adhesive which ex.. |
|||
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
3M 9738 Double Coated Splicing Tape 3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres.. |
|||
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
3M 3311 General Purpose Aluminum Foil Tape Ul 723 listedInformation provided by 3M |
|||
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
3M 9737R Double Coated Splicing Tape 3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres.. |
|||
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
Chesterton 651 Detergent Lubricating Oil Description: Chesterton® 651 Detergent Lubricating Oil is the plant-wide product of choice for superior-quality, low-viscosity, industrial lubricating needs. It is a cost-effective oil with high de.. |
|||
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
Chesterton 652 Pneumatic Lubricant & Conditioner Description: Chesterton® 652 Pneumatic Lubricant & Conditioner is a high performance, low viscosity, lubricating formula designed to creep into the internal workings of air tools, reduce wear and e.. |