Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | |
Parker Chomerics CHO-BOND 360-208 Conductive Epoxy Low cost, electrically conductive epoxy adhesive that combines the good adhesive characteristics as epoxy, and the superior electrical conductivity of silver. It is recommended as a thermo-setting E.. |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | |
Parker Chomerics CHO-BOND 584-208 Conductive Adhesive Two-component, highly conductive adhesive system that combines the good adhesive characteristics of epoxy with the superior conductivity of silver. In addition to being available in bulk form, the m.. |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | |
Parker Chomerics CHO-BOND 592 Conductive Epoxy Highly conductive silver-filled epoxy adhesive which combines the best properties of metals and organics. This two-component system is unique in that it combines long pot life, good electrical condu.. |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | |
Parker Chomerics CHO-BOND® 592 Conductive Adhesive Description: CHO-BOND® 500 Series Adhesive/Sealant Compounds; These pure silver-filled materials are used where tight tolerances require thin bond lines. Various cure cycles are available, and the .. |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | Silicone Version |
Parker Chomerics COMBO® and COMBO® Strip Gasketing Wire Mesh EMI Gasket Selection Guide Construction: Formed Knitted Wire Strips in Parallel with Elastomer Strips; or Die-Cut GasketsAvailable Forms: Strips, Gaskets Made by Joining Strips.Standard Metals Available in EMI Portion: Monel .. |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | Silicone Version |
Parker Chomerics Frame Gasketing Wire Mesh EMI Gasket Selection Guide Construction: Formed Knitted Wire Strips Clamped in Aluminum ExtrusionsAvailable Forms: Strips, Fab. Lengths, Frames with Joined EMI Strips..Standard Metals Available in EMI Portion: Monel FerrexInf.. |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | Silicone Version |
Parker Chomerics PORCUPINE METALASTIC® Gasketing Wire Mesh EMI Gasket Selection Guide Construction: Expanded Metal in ElastomerAvailable Forms: Sheets, Die-Cut GasketsStandard Metals Available in EMI Portion: Monel AluminumInformation provided by Chomerics |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | Cured |
Parker Chomerics Tecknit® 72-00008 Silver-Filled Epoxy System Description: This commercial grade, conductive epoxy is designed for use in bonding applications where good conductivity is required. When mixed in a ratio of 1:1.4 by volume or weight, the two comp.. |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | Cured |
Parker Chomerics Tecknit® 72-08116 Silver-Filled Epoxy System Description: This is a silver filled epoxy system designed for maximum performance and lowest volume resistivity. It is easily mixed 1:1 by volume or weight, from the two one-ounce jars. Its consist.. |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | |
Parker Chomerics CHO-BOND 360-20 Conductive Epoxy Low cost, electrically conductive epoxy adhesive that combines the good adhesive characteristics as epoxy, and the superior electrical conductivity of silver. It is recommended as a thermo-setting E.. |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | Silicone Version |
Parker Chomerics COMBO® Gaskets Wire Mesh EMI Gasket Selection Guide Construction: Formed Knitted Wire Strips in Parallel with Elastomer Strips; or Die-Cut GasketsAvailable Forms: Die-Cut Elastomer with Joined EMI Strips.Standard Metals Available in EMI Portion: Mone.. |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | Silicone Version |
Parker Chomerics MESH STRIP™ (Elastomer Core) Wire Mesh EMI Gasket Selection Guide Construction: Knitted wire mesh over elastomer stripAvailable Forms: Strips, Gaskets Made by Joining Strips, Clip-On Strips.Standard Metals Available in EMI Portion: Monel Ferrex, Aluminum.Informati.. |
|||
Minimum Service Temperature, Air | -62.0 - -48.0 °C | -79.6 - -54.4 °F | Average value: -57.3 °C Grade Count:9 |
Overview of materials for Silicone, RTV, Construction Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Construction Grade". Each property range of values reported is minimum and maximum values.. |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | Elasticity is retained to this temperature. |
Momentive Performance Materials 1200® Construction Sealant One-part, premium glazing sealant for structural as well as general purpose glazing. Cure Method: Acetoxy. Tack-free time |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | Elasticity is retained to this temperature. |
Momentive Performance Materials Contractors SCS 1000® Construction Sealant One-part, for general purpose glazing and sealing applications. Cure Method: Acetoxy. Tack-free time |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | Elasticity is retained to this temperature. |
Momentive Performance Materials Sanitary 1700â„¢ Construction Sealant One-part, mildew-resistant sealant for ceramic tile, showers, tubs, and plumbing fixtures. Cure Method: Acetoxy. Tack-free time |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | Elasticity is retained to this temperature. |
Momentive Performance Materials Ultraglaze® 4000 Construction Sealant High strength, one-part structural glazing/weathersealing system. Cure Method: Alkoxy (Neutral). Tack-free time 2 to 5 hr. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silicones.GE Sili.. |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | Elasticity is retained to this temperature. |
Momentive Performance Materials Ultraglaze® SSG 4000AC Construction Sealant High strength, one-part, accelerated-cure structural glazing/weathersealing system.Cure Method: Alkoxy (Neutral). Tack-free time 1 hr. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silico.. |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | Elasticity is retained to this temperature. |
Momentive Performance Materials Silglaze® II Construction Sealant One-part, for channel, stop, and butt glazing. Primerless adhesion properties. Cure Method: Methoxy (Neutral). Tack-free time 0.5 hr. Peel Strength 30 lb/in.; Sag/slump 0.1 in.Data provided by .. |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | |
Tra-Con Tra-Bond 872-7TN1 Flexible Thixotropic Epoxy Adhesive TRA-BOND 872-7TN1 is a flexible thixotropic epoxy. The high viscosity and long worklife make this material easy to handle. Also, the high thermal conductivity makes this product ideal for electronic.. |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | |
Dow Corning 735 OIL RESISTANT SEALANT Black RTV that resists most oils, coolants, etc.Information provided by Dow Corning |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | |
Dow Corning 738 ELECTRICAL SEALANT. WHITE Durable general purpose sealant/adhesive for a wide variety of bonding and sealing applications. Can be used in applications where mil spec is required.Information provided by Dow Corning |
|||
Minimum Service Temperature, Air | -62.0 °C | -79.6 °F | Silicone Version |
Parker Chomerics POLASHEET® Metal EMI Gasket Description: POLASHEET gasketing are composite EMI shielding and weather sealing materials. Either solid or sponge silicone may be specified as the weather seal. In POLASHEET gasketing individual mo.. |