Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Polikim ULPOLEN® 300 UHMWPE Standard Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Precision Polymer Engineering R50D Natural Rubber Natural Rubber, 45-55 °IRHD. Formulated to Defence Standard 93-30, Type QX, Grade 50 (NRQX50).Applications: Natural rubber offers low compression set, high tensile strength, high resilience and ex.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Precision Polymer Engineering R80Z Natural Rubber Natural Rubber, 75-85 °IRHD. Formulated to meet BS1154 Grade Z80. In accordance with BS1154 this material is based on high-quality plantation (Hevea) rubber, reinforced with carbon black.Applicati.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Cured |
Resin Technology Group UV-S-2051 High Impact, UV Curable Plastic Bonder UV S-2051 is a general purpose, fast cure response, high thermal-shock resistant, UV curing adhesive designed for use in a variety of applications including chip bonding, laminating, tacking, and se.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Manifattura Cattaneo PEEK Polyetheretherketone Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Continuous; DIN 52612 |
Isoflon POM H Polyacetal H Good optical propertiesHigh UV resistanceAbsorbs little moistureInformation provided by Isoflon. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Retraction Temperature, ARM 201 fluid immersion, 70 hrs. at 275°F; ASTM D1329 |
Freudenberg Simrit N456 Nitrile Elastomer (NBR) General Purpose; Internal Lubricant. Inferior resistance to ozone, sunlight and natural aging; poor resistance to oxygenated solvents. All testing done on AS568-214 size o-rings |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Continuous useful temperature. |
Momentive Performance Materials RTV6196 Clear Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Seals Eastern 7346 Extreme Low Temperature Service Rubber HNBR for cold temp (-50°C) and/or aqueous serviceInformation provided by Seals Eastern. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Goodfellow Polyaramid/Vinylester Composite Tube or Rod Information provided by Goodfellow. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Tra-Con Tra-Cast 3110 Low Density Epoxy Casting System TRA-CAST 3110 is a unicellular, low density, syntactic-foam epoxy resin casting system of medium viscosity that easily handles, mixes and cures at room temperature. Developed for industrial encapsul.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Trelleborg R547 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Trelleborg R650 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 400701S SBS Based Material, 70A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 500900S SEBS Based Material, Unfilled Qualities, 90A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 502450S SEBS Based Material, Unfilled Qualities, 45A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 502800S SEBS Based Material, Unfilled Qualities, 80A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 502900S SEBS Based Material, Unfilled Qualities, 90A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 600700S SEBS Based Material, Filled Qualities, 70A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 602450S SEBS Based Material, Filled Qualities, 45A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 602750S SEBS Based Material, Filled Qualities, 75A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 660500S SEBS Based Material, Semi-Filled Qualities, 50A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Mediprene™ 660420M TPE, Medical Applications, 42A Hardness All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications. In both medical and food contact areas, high application demands are found, such as:Low e.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | JIS-K-6723 |
Denka REOMER G G5377 Thermoplastic Elastomer, For Extrusion Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 600550S SEBS Based Material, Filled Qualities, 55A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Atom Adhesives AA-DUCT 902 Epoxy Adhesive and Coating AA-DUCT 902 is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value of.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Recommended |
Nye Lubricants 363 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Rogers Corporation Bisco® A2 R 3.0 Engineered Solid Silicone Mass Layer, Fiberglass Reinforced Sound Barrier BISCO® A2 Fiberglass Reinforced Sound Barrier provides a similar level of sound absorption and flame resistance as the non-reinforced A2 Sound Barrier with the addition of increased tensile and tea.. |