Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -48.0 °C | -54.4 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering E70Z Ethylene Propylene Rubber Peroxide cured, grey Ethylene Propylene Terpolymer, 65-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Specially formulated for sealing applications involving high voltage electri.. |
|||
Minimum Service Temperature, Air | -48.0 °C | -54.4 °F | Recommended |
Nye Lubricants 791B (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -48.0 °C | -54.4 °F | Retraction Temperature, TR10; ASTM D1329 |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with Sundex 790 MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Minimum Service Temperature, Air | -48.0 °C | -54.4 °F | Elasticity is retained to this temperature. |
Momentive Performance Materials Silpruf® Construction Sealant One-part, for weatherseals, structural glazing, and general purpose sealing. Cure Method: Alkoxy (Neutral). Tack-free time 5 to 10 hr.; Peel Strength 55 lb/in.; Sag/slump 0.1 in.Data provided by the.. |
|||
Minimum Service Temperature, Air | -48.0 °C | -54.4 °F | Elasticity is retained to this temperature. |
Momentive Performance Materials UltraPruf® SCS 2300 Construction Sealant One-part, for concrete, masonry, and stone. Matte finish. Cure Method: Alkoxy (Neutral); Tack-free time 5 to 10 hr. Peel Strength 55 lb/in. Sag/slump 0.1 in.Data provided by the manufacturer, GE.. |
|||
Minimum Service Temperature, Air | -48.0 °C | -54.4 °F | Retraction Temperature, TR10; ASTM D1329 |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with Cumar P-10 MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Minimum Service Temperature, Air | -48.0 °C | -54.4 °F | Retraction Temperature, TR10; ASTM D1329 |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with Sundex 790 MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Minimum Service Temperature, Air | -48.0 °C | -54.4 °F | JIS-K-6723 |
Denka REOMER G G5048 Thermoplastic Elastomer, For Extrusion Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |
|||
Minimum Service Temperature, Air | -48.0 °C | -54.4 °F | JIS-K-6723 |
Denka REOMER G G5059 Thermoplastic Elastomer, For Extrusion Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |
|||
Minimum Service Temperature, Air | -48.0 °C | -54.4 °F | JIS-K-6723 |
Denka REOMER G G8053 Thermoplastic Elastomer, For Injection Molding Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |
|||
Minimum Service Temperature, Air | -48.0 °C | -54.4 °F | |
3M Scotchrap™ 50 Tape 3M™ Scotchrap™ Tapes 50 and 51 are tough, polyvinyl chloride based tapes with special high tack adhesives formulated to resist corrosion of metal piping systems above and below ground, fittings an.. |
|||
Minimum Service Temperature, Air | -48.0 °C | -54.4 °F | |
3M Scotchrap™ 51 Tape 3M™ Scotchrap™ Tapes 50 and 51 are tough, polyvinyl chloride based tapes with special high tack adhesives formulated to resist corrosion of metal piping systems above and below ground, fittings an.. |
|||
Minimum Service Temperature, Air | -48.0 °C | -54.4 °F | Elasticity is retained to this temperature. |
Momentive Performance Materials Ultraglaze® 4400 Construction Sealant High strength, two-part structural glazing system. Cure Method: Condensation. Tack-free time 3 hr. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of .. |
|||
Minimum Service Temperature, Air | -48.0 °C | -54.4 °F | Retraction Temperature, TR10; ASTM D1329 |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with Cumar P-10 MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |