Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -47.8 °C | -54.0 °F | |
Arlon 920-410C##FR-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape
(discontinued **) Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Brown, Rectangular cross-section, Self-fu.. |
|||
Minimum Service Temperature, Air | -47.8 °C | -54.0 °F | |
Arlon 920-05B##-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 0.5” Wide Rectangular 0.5 inch wide, 20 mil thick, Black, Rectangular cross-section, Sel.. |
|||
Minimum Service Temperature, Air | -47.8 °C | -54.0 °F | |
Arlon 920-05C##FR-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 0.5” Wide Rectangular .0.5 inch wide, 20 mil thick, Black, Rectangular cross-section, Se.. |
|||
Minimum Service Temperature, Air | -47.8 °C | -54.0 °F | |
Arlon 920-10B##-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Brown, Rectangular cross-section, Self-fu.. |