Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | >= -29.0 °C | >= -20.2 °F | optimum performance range |
Sorbothane Polyurethane Damping Material, 30 Durometer Sorbothane® is a thermoset, polyether-based polyurethane viscoelastic material that combines high energy absorption with faultless memory. Sorbothane turns mechanical energy into heat. As the m.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | See Note 1. |
ChevronTexaco Coupling Grease NLGI Grade 0/1 Texaco Coupling Grease delivers value through:Superior film strength — Formulated with a high viscosity base oil and polymer for superior film strengthLittle to no oil separation in high-speed coup.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M 7046 Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products 7046 and 7053 are durable, high performance materials that offer excellent durability and moisture resistance. These vinyl label stocks utilize.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FL00700N Lexan Label Product 3M™ Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P1212, which is a high .. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FL015 Lexan Label Product 3M™ Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P1212, which is a high .. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FM019602 MC Polyester Label Products 3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FM023402 Clear Polyester Label Products 3M™ Clear Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FM030 Indoor UL Recognized Clear Polyester Label Products on 3M™ Indoor UL Recognized Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for dem.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FM052 Indoor UL Recognized Brite Silver Polyester Label Products 3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FM118B Indoor UL Recognized MC Polyester Label Products 3M™ Indoor UL Recognized MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These po.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FM12B Indoor UL Recognized White Polyester Label Products 3M™ Indoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ A.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FM282 Indoor UL Recognized White Polyester Label Products 3M™ Indoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ A.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FP011902 Removable White Polypropylene Label Product 3M™ Removable White Polypropylene Label Product FP011902 is a glossy white opaque material that offers excellent durability and moisture resistance. This label product utilizes 3M™ Adhesive RMR10,.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FP02680N White Polypropylene Label Products 3M™ White Polypropylene Label Products FP02680 is a white opaque material that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1480, which is a high .. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FP083 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FP102 Clear Polypropylene Label Product 3M™ Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1410, which is a general purpose permanent tackified acrylic t.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FV291 White Vinyl Label Products 3M™ White Vinyl Label Products FV291 and FV292 are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl label products utilize 3M™ Adhesive P14.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FV292 White Vinyl Label Products 3M™ White Vinyl Label Products FV291 and FV292 are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl label products utilize 3M™ Adhesive P14.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FV392 Removable White Vinyl Label Products 3M™ Removable White Vinyl Label Products FV1172 and FV392 are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive .. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FVT40 Tire Label Product 3M™ Tire Label Products utilize a flexible and conformable white vinyl labelstock that offers durability, moisture resistance, and dimensional stability. 3M™ Adhesive G1120, a rubber-based aggress.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FVT44 Tire Label Product 3M™ Tire Label Products utilize a flexible and conformable white vinyl labelstock that offers durability, moisture resistance, and dimensional stability. 3M™ Adhesive G1120, a rubber-based aggress.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Application |
3M OFM0101 Outdoor UL Recognized Polyester Overlaminate Label Products 3M™ Outdoor UL Recognized Polyester Overlaminate Label Products are durable high performance clear materials that offer excellent thermal stability, abrasion and moisture resistance. These polyeste.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M OFM0502 Outdoor UL Recognized White Polyester Label Product 3M™ Outdoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ .. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M OFM1602 Outdoor UL Recognized Clear Polyester Label Product 3M™ Outdoor UL Recognized Clear Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ .. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | |
3M 32666 Tan Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FM239 Indoor UL Recognized Matte Clear Polyester Label Products 3M™ Indoor UL Recognized Matte Clear Polyester Label Products FM23N, FM232 and FM239 are durable, high performance materials that offer excellent thermal stability and moisture resistance. These po.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FP025409 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are clear materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1480, which is a high performance tac.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M OFM0403 Outdoor UL Recognized White Polyester Label Product 3M™ Outdoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ .. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M OFM0709 Outdoor UL Recognized Brite Silver Polyester Label Products 3M™ Outdoor UL Recognized Brite Silver Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FV0146N Soft Clear Vinyl Label Products 3M™ Soft Clear Vinyl Label Products are flexible, conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high.. |