Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | 149 °C | 300 °F | |
Monmouth Rubber & Plastics Durafoamâ„¢ C41 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Minimum Service Temperature, Air | 149 °C | 300 °F | |
Monmouth Rubber & Plastics Durafoamâ„¢ C42 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Minimum Service Temperature, Air | 149 °C | 300 °F | |
Monmouth Rubber & Plastics Durafoamâ„¢ C43 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Minimum Service Temperature, Air | 149 °C | 300 °F | |
Monmouth Rubber & Plastics Durafoamâ„¢ C44 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Minimum Service Temperature, Air | 149 °C | 300 °F | |
Monmouth Rubber & Plastics Durafoamâ„¢ C45 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Minimum Service Temperature, Air | 149 °C | 300 °F | |
Monmouth Rubber & Plastics Durafoamâ„¢ P493SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Minimum Service Temperature, Air | 149 °C | 300 °F | |
Monmouth Rubber & Plastics Durafoamâ„¢ P497SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Minimum Service Temperature, Air | 149 °C | 300 °F | Lower limit of working range |
Heatbath/Park Low Temperature Draw Salt Quenching and Tempering Salt A eutectic mixture offering the lowest melting point and a wide working range. Formulated per MIL-S-10699-B, Class 1 (275 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical... |
|||
Minimum Service Temperature, Air | 149 °C | 300 °F | Lower limit of working range |
Heatbath/Park Scale Kleen 1259 Descaling Salt A highly alkaline and oxidizing salt bath used specifically as a low temperature bath for descaling titanium and titanium alloys.Information provided by Heatbath Corporation - Park Metallurgical. |
|||
Minimum Service Temperature, Air | 149 °C | 300 °F | Lower limit of working range |
Heatbath/Park Thermo-Quench Oil A "hot" or "marquenching" oil offering excellent thermal stability, high flash point and fast quenching rate.Information provided by Heatbath Corporation - Park Metallurgical. |
|||
Minimum Service Temperature, Air | 149 °C | 300 °F | Lower limit of working range |
Heatbath/Park Thermo-Quench Quenching and Tempering Salt Most widely used quench salt for more than a decade. This eutectic nitrate/nitrite mixture is highly recommended for the interrupted or isothermal quenching of austenitized steels. Slightly higher,.. |
|||
Minimum Service Temperature, Air | 149 °C | 300 °F | Lower limit of working range |
Heatbath/Park Parcure 275 Rubber Cure Salt Nitrate/Nitrite Salt. An eutectic mixture offering the lowest possible melting point and the widest working range. (275 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical. |
|||
Minimum Service Temperature, Air | 149 °C | 300 °F | Lower limit of working range |
Heatbath/Park Partherm 290 Heat Transfer Salt The most widely used heat transfer salt. It is an eutectic mixture with a low melt point and a wide working range. (290 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical. |