Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | 121 °C | 250 °F | |
Monmouth Rubber & Plastics Durafoamâ„¢ C41NBR Nitrile Rubber Information provided by Monmouth Rubber & Plastics Corp. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | |
Monmouth Rubber & Plastics Durafoamâ„¢ C42NBR Nitrile Rubber Information provided by Monmouth Rubber & Plastics Corp. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | |
Monmouth Rubber & Plastics Durafoamâ„¢ C43NBR Nitrile Rubber Information provided by Monmouth Rubber & Plastics Corp. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | |
Monmouth Rubber & Plastics Durafoamâ„¢ DK1111 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | |
Monmouth Rubber & Plastics Durafoamâ„¢ DK2121 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | |
Monmouth Rubber & Plastics Durafoamâ„¢ DK3131 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | |
Monmouth Rubber & Plastics Durafoamâ„¢ DK5151 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | Lower limit of working range |
Heatbath/Park Marquench Oil M An accelerated quench oil designed for applications at 250° to 350°F. The use of this "hot" oil is commonly encountered in carburizing and carbonitriding furnaces or where parts are prone to .. |
|||
Minimum Service Temperature, Air | 121 °C | 249 °F | Lower limit of working range |
Heatbath/Park Partherm 430 Heat Transfer Salt A popular heat transfer salt for use in the higher temperature ranges. It is more inert to ferrous alloys than Partherm 290 or 350 and considerably lower in cost. Its heat capacity and thermal cond.. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | Short term |
3M 12028 Black 1/8" (3.2 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | Short term |
3M 12032 Black 3/32" (2.4 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | Short term |
3M 12038 Black 3/8" (9.5 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | Short term |
3M 12049 Black 3/8" (9.5 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | Short term |
3M 12050 Black 1/2" (12.7 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | Short term |
3M 12062 Black 3/32" (2.4 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | Short term |
3M 12026 Black 1/16" (1.6 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | Short term |
3M 12034 Black 1/4" (6.4 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | Short term |
3M 12036 Black 3/16" (4.8 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | Short term |
3M 12046 Black 1/16" (1.6 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | Short term |
3M 12048 Black 1/8" (3.2 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | Short term |
3M 12054 Black 1/4" (6.4 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | Short term |
3M 12056 Black 3/16" (4.8 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | Short term |
3M 12030 Black 1/2" (12.7 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 121 °C | 250 °F | |
Monmouth Rubber & Plastics Durafoam™ DK4141 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |