Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Garlock 5500 Compressed Inorganic Fiber Gasketing, Nitrile Binder Inorganic fibers with a nitrile binder.Inorganic fiber gasketing offers excellent thermal stability with minimal weight lossReduced creep relaxation and improved torque retention provide optimal sea.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Garlock MULTI-SWELLâ„¢ 3760 Compressed Aramid Fiber Gasketing Aramid fibers with a proprietary rubber binder.Creates compressive load in light weight flanges in oil and water serviceTwice as compressible as standard fiber gasketsSeals with low load and irregul.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Garlock MULTI-SWELLâ„¢ 3760-U Compressed Aramid Fiber Gasketing Aramid fibers with a proprietary rubber binder.Creates compressive load in light weight flanges in oil and water serviceTwice as compressible as standard fiber gasketsSeals with low load and irregul.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Greene Tweed WR™ FP100 Polyketone, Reinforced Greene Tweed’s WR® FP100, a reinforced compression-molded polyketone, offers excellent wear resistance with FDA compliance. The typical properties and physical characteristics of WR FP100 m.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Garlock 9800 Compressed Carbon Fiber Gasketing, SBR Binder Carbon fibers with a SBR binder.Carbon fiber gasketing excels in harshest conditions- intense heat, high pressure, saturated steam and hot oilsLaboratory tested for fire safetyMaintains effective se.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain Chemlam® SGC6-06 Copper Adhesive Tape Description: Chemlam® Copper SGC6 is fiberglass fabric impregnated with PTFE (polytetrafluoroethylene) dispersion, laminated to PTFE film and coated with high-temperature, pressure-sensitive sili.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® 2042-5 Skived PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® 2265-2 Extruded PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® 2345-5 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® 280-6(R) Roll Covering Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® 2975-8R Glass-Silicone Backing Silicone Adhesive Pressure Sensitive Tape Description: Silicone glass provides temperature resistance from -85°F to +500°F (-62°C to +260°C) and exceptional tensile strength and abrasion resistance. Applications include thermal .. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® C Film Backing Silicone Adhesive Pressure Sensitive Tape Description: FEP film is used for applications requiring optical clarity, quick release, and abrasion resistance. FEP film applications include high temperature coil and capacitor wrapping, composit.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® K104 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® M66 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® SG15-06(R) High Performance Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® SG26-06(R) Primary Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® SG26-10(R) Primary Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® SGB6-10(R) CHEMLAM Brown Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® T Skived PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Master Bond EP21TDC-4ND Two component, highly flexibilized epoxy for bonding, sealing and coating Product Description: Master Bond EP21TDC-4ND is a two component, very flexible epoxy system for high performance bonding, sealing and coating with a non-drip consistency. It has a one to four mix ra.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Master Bond EP46HT-1 Epoxy For Serviceability Up To 600°F Description: Master Bond EP46HT-1 is a two component epoxy system for high performance structural bonding and sealing suitable for applications where resistance to temperatures from -100°F to +550°.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Master Bond Supreme 11ANHT Fast Curing Epoxy Paste System Description: Master Bond Polymer System SUPREME 11ANHT is a two component epoxy resin system for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevat.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Master Bond Supreme 11AO Electrically Isolating Adhesive and Sealant Description: Master Bond Polymer System SURPEME 11AO is a two component epoxy resin system for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevated.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Master Bond Supreme 33CLV Two Component, Room Temperature Curing Toughened Epoxy Master Bond Polymer System Supreme 33CLV is a special, room temperature curing, toughened epoxy adhesive/sealant, featuring exceptionally high temperature resistance. This innovative system has outs.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -99.9 °F | |
Arlon 0.015" (0.381 mm) Primerless Thermabond® Uncured Silicone (99990A015) 0.015 in., ±0.001 (0.38 mm, ±0.038) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.015 in ±0.001(0.38 mm ± 0.038).. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Arlon R30370A008 0.008" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.001" FEP FilmSide 1: Unsupported/Uncured Silicone RubberSubstrate: 0.003" PTFE coated FiberglassThis data represents typical values for the production material a.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Arlon Thermabond® T20 (99710W015) 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: 15 mil thick Thermabond® T20 electrically insulating electronic adhesive.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Pri.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Master Bond Supreme 46HT-2ND2 Two Component, Non-Drip, Toughened, Epoxy Adhesive Master Bond Polymer Supreme 46HT-2ND2 is a two component, non-drip, epoxy adhesive featuring an attractive balance of superior shear and peel strengths for high performance structural bonding suitab.. |