Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 101 Cyanoacrylate, Wicking Viscosity PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 105 Cyanoacrylate, for difficult rubbers PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 170 Cyanoacrylate, gap filling PERMABOND® 170 is a methyl cyanoacrylate adhesive. It is a single part, high viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. Permabond 170 w.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 268 Cyanoacrylate, General purpose PERMABOND® 268 is a medium-high viscosity cyanoacrylate for large gap fill applications. Permabond® 268 provides faster set times and improved gap-filling capability compared to conventional cyano.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 940 Cyanoacrylate, low odor PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 799 Cyanoacrylate, Surface insensitive PERMABOND® 799 is a high viscosity cyanoacrylate that combines fast cure with the ability to cure through a large gap. Plastics, metals, ceramics and elastomers are also rapidly bonded. The fast cu.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 801 Cyanoacrylate, High Temperature PERMABOND® 801 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 820 Cyanoacrylate, High Temperature PERMABOND® 820 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 920 Cyanoacrylate, High temperature PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 931 Cyanoacrylate PERMABOND 931 is a low odor, nonfogging, nonfrosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 932 Cyanoacrylate PERMABOND 932 is a low odor, nonfogging, nonfrosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT is an one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation prof.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond EP21LV35Med Two Component, Flexible USP Class VI Epoxy System Master Bond Polymer System EP21LV3/5Med is a two part, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting that cures flexible. It cures readil.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond EP21TP-2 Two Component Polysulfide Epoxy Adhesive and Sealant Master Bond Polymer Adhesive EP21TP-2 is a two component polysulfide/epoxy based adhesive/sealant formulated to cure at room temperature or more rapidly at elevated temperatures, with a 100 to 100 m.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond EP30-3LO Highly versatile, two part epoxy system for bonding, coating, sealing and casting Master Bond EP30-3LO is a two component epoxy system featuring a combination of optical clarity and light transmission, good glass transition temperature (Tg), great chemical resistance along with p.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond EP37-3 Optically Clear, Impact Resistant Two Component Epoxy Master Bond Polymer System EP37-3 is a low viscosity, resilient, optically clear two component epoxy resin system designed for high performance bonding, coating and casting applications. As an adhes.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond EP45HTMED Epoxy Resists Radiation and Steam Sterilization Description: Master Bond Polymer System EP45HTMED is a two component heat cured epoxy system for high performance structural bonding, sealing, coating and casting. It is especially designed for the .. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond EP65ND Fast Curing, High Shear Strength Epoxy This two component adhesive system is formulated to cure quickly at ambient temperatures e.g. 8-10 minutes, shorter lives at higher temperatures for maximum bond strength. Tensile lap shear strength.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond Supreme 33 High Temperature Resistant, Structural Adhesive Description: Master Bond Polymer System Supreme 33 is a unique, room temperature curing, toughened epoxy adhesive/sealant, offering high temperature resistance. This innovative system offers high bo.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond UV15X-2GT One Component, UV Curable Glob Top Compound Master Bond Polymer System UV15X-2GT is a one component, easily processable, UV curable glob top, featuring exceptional durability and chemical resistance. UV15X-2GT is a thixotropic paste that hand.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond UV15X-6MED-2 UV Curable Compound for Medical Applications Description: Master Bond Polymer System UV15X-6MED-2 is a newly developed one component clear, non-yellowing, UV curable urethane elastomer system possessing high flexibility and outstanding abrasio.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 792 Cyanoacrylate, Surface insensitive PERMABOND® 792 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 941 Cyanoacrylate, low odor PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 943 Cyanoacrylate, low odor PERMABOND 943 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Permabond 947 Cyanoacrylate, low odor PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Minimum Service Temperature, Air | -62.2 °C | -80.0 °F | |
Master Bond EP30M4LV Chemically Resistant, Low Viscosity Adhesive Description: Master Bond EP30M4LV is a two component, low viscosity epoxy system for high performance bonding, sealing and encapsulation. This system features a forgiving 100 to 60 mix ratio by weig.. |