Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -59.0 °C | -74.2 °F | Cured |
Parker Chomerics Tecknit CON/RTV-I One Part: Silver-Filled Silicone RTV Description: TECKNIT CON/RTV-I system is a pure silver loaded, one component RTV silicone adhesive sealant. It is ready to use without mixing and cures quickly at room temperature on exposure to moi.. |
|||
Minimum Service Temperature, Air | -59.0 °C | -74.2 °F | |
Dow Corning 1890 PROTECTIVE COATING Silicone RTV in solvent dispersionInformation provided by Dow Corning |