Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 180 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 373 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 723S-MS (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 825-1 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
Parker Chomerics CHO-SHIELD® 4925 Conductive Coating Conductive Coating. CHO-SHIELD 4925 silver and nickel-filled conductive acrylic coating is intended for EMI shielding commercial thermoplastic housings. Its unique solvent system has been formulated.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Cured |
Parker Chomerics Tecknit® 73-00081 Electrically Conductive Acrylic and Polyurethane Paint Description: TECKNIT manufactures a highly conductive acrylic and polyurethane paints filled with silver. These coatings provide a cost effective method for shielding and grounding plastic enclosure.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Cured |
Resin Technology Group UV-422 Flexible, UV Curing Sealant UV 422 is a semi-flexible, UV curing adhesive that can be used in a wide variety of potting, sealing, tacking and bonding applications. High strength bonds are formed to PVC and polycarbonate substr.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 706D-UV (IG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Recommended |
Nye Lubricants 902B (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
Permabond 798 Cyanoacrylate, Surface insensitive PERMABOND 798 is a high viscosity cyanoacrylate that combines fast cure with the ability to cure through a large gap. Plastics, Metals, Ceramics and elastomers are also rapidly bonded. The fast cu.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
Permabond 930 Cyanoacrylate PERMABOND 930 is a low odor, nonfogging, nonfrosting cyanoacrylate. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesives on hot and humid days, is eliminated. The .. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
Momentive Performance Materials RTV8111 Silicone Rubber Compounds for Potting, Encapsulating and Sealing RTV8111, RTV8112 and RTV8262 silicone rubber compounds are two-part silicone elastomers supplied in ready-to-use matched kits containing a base compound and curing agent.Mechanical and electrical pr.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Continuous useful temperature. |
Momentive Performance Materials RTV8112 White General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
Tra-Con Tra-Duct 2705 Room Temperature Conductive Nickel Epoxy Adhesive TRA-DUCT 2705 is an electrically conductive nickel filled epoxy adhesive recommended for electronic bonding, sealing, and EMI-RFI shielding applications. This two-part smooth paste formulation is fr.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M 363L Specialty Foil Tape Linered version of 363Information provided by 3M |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | cured 14 days @ 50% RH |
3M AC-350 Class A-1 Aerospace Sealant 3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | cured 14 days @ 50% RH |
3M AC-350 Class A-2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | MIL-PRF-81733D |
3M AC-665 Class C-48 Aerospace Sealant 3M Aerospace Sealant AC-665 Class C are two-part, manganese-cured, chromate containing, corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corros.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | cured 14 days @ 50% RH |
3M AC-730 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | cured 14 days @ 50% RH |
3M AC-736 B-2 Aerospace Sealant 3M Aerospace Sealant AC-736 B-2 is a non-chromate corrosion inhabiting sealants, fast cure, low density two-component, manganese dioxide cure, polysulfide fuselage sealant. These Sealants act as an .. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Continuous |
3M Scotch-Weld™ HT700 High Temperature Instant Adhesive 3M™ Scotch-Weld™ High Temperature Instant Adhesives provide superior performance for demanding applications where high temperatures, thermal cycling, or shock resistance is required. HT700 is a me.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M Scotch-Weld™ LO100 Low Odor Instant Adhesive 3M™ Scotch-Weld™ Low-Odor Instant Adhesives are formulated to have low volatility while maintaining bonding of a wide rage of materials. Low volatility means that these products are not only low o.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M 5481 PTFE Skived Film Tape 3M™ PTFE Skived Film Tape 5481 is a film backing with a silicone adhesive.Information provided by 3M |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M Scotch-Weld™ SF100 Super Fast Instant Adhesive 3M™ Scotch-Weld™ Super Fast Instant Adhesives rely less on surface moisture for cure speed than standard cyanoacrylates. They are designed to join together difficult-to-bond plastics and rubbers, .. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M Scotch-Weld™ SI Gel Surface Insensitive Instant Adhesive 3M™ Scotch-Weld™ Surface Insensitive Adhesives bond rough, porous, contaminated, and acidic substrates including wood, cardboard, veneer, fabric, cork, and leather. SI Gel (formerly SB09) is a fas.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M Scotch-Weld™ SI100 Surface Insensitive Instant Adhesive 3M™ Scotch-Weld™ Surface Insensitive Adhesives bond rough, porous, contaminated, and acidic substrates including wood, cardboard, veneer, fabric, cork, and leather. SI100 is a low viscosity produc.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
3M Scotch-Weld™ PS67 Pipe Sealant Anaerobic Adhesives 3M™ Scotch-Weld™ Pipe Sealant Anaerobic Adhesives are one-component anaerobic sealants that cure and seal hydraulic and pneumatic pipes and fittings to withstand high temperatures and pressures. P.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | Intermittent |
3M Scotch-Weld™ RT3500B Rubber-Toughened Instant Adhesive 3M™ Scotch-Weld™ Rubber Toughened Instant Adhesives are formulated with a unique elastomer that maximizes impact, vibration, peel, and thermal cycling resistance while providing tough flexible bon.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | cured 14 days @ 50% RH |
3M AC-240 Class B-4 Aerospace Sealant 3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan.. |
|||
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F | |
ACC QSil 60 QSI Quantum Silicones 50 Durometer Condensation Cure for Potting QSil 60 is a red, high temperature, self-leveling, two-component, silicone material primarily used for potting applications. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section .. |