Polymer Property : Minimum Service Temperature, Air = -48.9 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -48.9 °C
-56.0 °F
Retraction Temperature, TR10; ASTM D1329
Freudenberg Simrit S310 Silicone Elastomer (VMQ)
General Purpose; AMS 3301; A-A-59588 (ZZ-R-765) Class 2A, 2B Grade 40; Good heat resistance. Poor resistance to abrasion, tear and cut growth; low tensile strength; inferior resistance to oil, gasol..
Minimum Service Temperature, Air -48.9 °C
-56.0 °F
T<sub>f</sub>; ASTM D746
Colorite Polymers Elastichem 5011TX-02 Vinyl Compound
Description: All components in Elastichem are sanctioned by the U.S. Food & Drug Administration for food packaging applications under Title 21 of the Code of Federal Regulations. For medical use, co..