Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -48.3 °C | -55.0 °F | |
ConocoPhillips Syncon® HP Synthetic Grease NLGI No. 1 Description: Conoco Syncon HP Synthetic Grease is a high-quality, synthetic polyalphaolefin (PAO) lithium grease developed to provide exceptional protection and corrosion resistance for bearings and.. |