Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Recommended |
Nye Lubricants 186 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
P & P Technology Chloroprene Neoprene Sponge Good resistance to heat and moderate chemicals and moderate resistance to oils. Has good characteristics to resist sea water, acids, fats, greases and many solvents. Neoprene has good ozone resistan.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Neoprene Version |
Parker Chomerics Frame Gasketing Wire Mesh EMI Gasket Selection Guide Construction: Formed Knitted Wire Strips Clamped in Aluminum ExtrusionsAvailable Forms: Strips, Fab. Lengths, Frames with Joined EMI Strips..Standard Metals Available in EMI Portion: Monel FerrexInf.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Neoprene Version |
Parker Chomerics MESH STRIP™ (Elastomer Core) Wire Mesh EMI Gasket Selection Guide Construction: Knitted wire mesh over elastomer stripAvailable Forms: Strips, Gaskets Made by Joining Strips, Clip-On Strips.Standard Metals Available in EMI Portion: Monel Ferrex, Aluminum.Informati.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
Chesterton 785 Parting Lubricant Description: Chesterton® 785 Parting Lubricant represents the newest generation of anti-seize compound. A proprietary blend of ultra-fine inorganic solid lubricants in a non-carbonizing, ashless sy.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
ChevronTexaco Delo® NLGI 0 Grease EP FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
ChevronTexaco Delo® NLGI 00 Grease EP FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | See Note 1. |
ChevronTexaco PremiumRB Texaco Premium RB delivers value through:Wide application range — Suitable for high rpm operation, operating temperatures ranging from -34°C to 177°C (-30°F to 350°F) and offers excellent rust .. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | JIS-K-6723 |
Denka VINYKON W2035 PVC, W grade for insulation, for sheaths A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | See Note 1. |
ChevronTexaco Starplex® NLGI Grade 1 Texaco Starplex greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protectio.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
ChevronTexaco Super Permalube® Grease FeaturesChevron Super Permalube Grease is a multipurpose automotive grease for applications requiring extreme pressure, wear, and rust protection as well as oxidation and water resistance. It is gre.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 3324 Copper Foil Tape EMI/RFI shieldingInformation provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 3340 HVAC Construction Aluminum foil tape, for use with rigid and flexible ducts. UL 181 A-P and 181 B-FX Listed.Information provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 3350 HVAC Construction Polypropylene tape for use with flexible ducts. UL 181 B-FX ListedInformation provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 3363 General Purpose Aluminum Foil Tape 40 lb natural kraft paper liner. Good for narrow slit rolls. UL 723 ClassifiedInformation provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 3380 HVAC Construction General purpose aluminum foil tape. Go to product for this market. UL 723 Classified.Information provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 33806 Premium Performance Aluminum Foil Tape High temperature acrylic adhesive of 425°FInformation provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 34383 General Purpose Aluminum Foil Tape General purpose aluminum foil tapeInformation provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 4380 General Purpose Aluminum Foil Tape 3M™ Aluminum Foil Tape 4380 is a general purpose aluminum foil tape offering a dead soft aluminum foil backing combined with an acrylic pressure sensitive adhesive.Information provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Service |
3M Bumpon™ SJ5816 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Service |
3M Bumpon™ SJ5904 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Service |
3M SJ5500 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Service |
3M SJ6344 Protective Product, Molded Shapes 3M Bumpon Protective Products SJ6344 is a pressure-sensitive adhesive-backed, molded polyurethane product. The Bumpon SJ6344 is called an Easy Slide Series because it incorporates a special abrasion.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 5421 Polyethylene Tape 3M™ Polyethylene Tape 5421 has a rubber adhesive which provides an excellent abrasion resistant surface.Information provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 9325 Squeak Reduction Tape 3M™ Squeak Reduction Tapes are a film tape for the automotive industry to help control squeaks and rattles due to vibration or wear of metal and plastic materials.Information provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 9343 Conformable Sound Management Film 3M™ Conformable Sound Management Film 9343 is designed for the reduction of noise, vibration, squeaks, and rattles in automotive interior applications. The currently available materials for these a.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Brittleness Temperature |
DuPont Performance Polymers Hypalon® 4085 Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound
(disc Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont .. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
Chesterton 783 ACR Anti-Seize Compound Description: Chesterton® 783 ACR represents the newest generation of anti-seize compound. A proprietary blend of ultra-fine inorganic solid lubricants, 783 ACR can be used under extremely severe co.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
Chesterton 785 FG Parting Lubricant Description: Chesterton® 785 FG Parting Lubricant represents the newest generation of food and pharmaceutical anti-seize compounds. A white soft-paste, formulated with proprietary blend of ultra-fi.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 33801 Premium Performance Aluminum Foil Tape High temperature acrylic adhesive of 425°F. UL 723 ClassifiedInformation provided by 3M |