Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
Chesterton 601 Chain Drive Pin & Bushing Lubricant Description: Chesterton® 601 Chain Drive Pin & Bushing Lubricant is and has been the premium quality light lubricant of choice in industry for over thirty years. This superior lubricant was special.. |
|||
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | See Note 1. |
ChevronTexaco 904 Grease NLGI Grade 1/2 Texaco 904 Grease is a calcium soap grease. It contains graphite which enhances its lubricity.Typical test data are average values only. Minor variations which do not affect product performance are .. |
|||
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | See Note 1. |
ChevronTexaco EP 1 Aluminum Complex Texaco Aluminum Complex EP 1 is manufactured using selected, high viscosity base oils, EP additives, rust and oxidation inhibitors. It has a high dropping point, which reduces the need for addition.. |
|||
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | See Note 1. |
ChevronTexaco Thermatex® EP NLGI Grade 1 Texaco Thermatex EP greases deliver value through:High temperature stability — Will not melt at high temperatures, but will remain in place on bearing surfaces and continue to provide excellent lub.. |
|||
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
3M 3334 Aluminum Foil/Scrim/PE Facing Tape 3M™ Aluminum Foil Tape 3334 has a high performance aluminum foil/bidirectional fiberglass scrim/polyethylene film laminate backing coated with a special pressure sensitive acrylic adhesive which ex.. |
|||
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
3M 9738 Double Coated Splicing Tape 3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres.. |
|||
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
3M 3311 General Purpose Aluminum Foil Tape Ul 723 listedInformation provided by 3M |
|||
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
3M 9737R Double Coated Splicing Tape 3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres.. |
|||
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
Chesterton 651 Detergent Lubricating Oil Description: Chesterton® 651 Detergent Lubricating Oil is the plant-wide product of choice for superior-quality, low-viscosity, industrial lubricating needs. It is a cost-effective oil with high de.. |
|||
Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
Chesterton 652 Pneumatic Lubricant & Conditioner Description: Chesterton® 652 Pneumatic Lubricant & Conditioner is a high performance, low viscosity, lubricating formula designed to creep into the internal workings of air tools, reduce wear and e.. |