Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -200 °C | -328 °F | |
Murtfeldt Murflor® Polytetrafluoroethylene Murflor® materials are suited to use in applications that require an excellent resistance to chemicals and heating steam. Murflor®’s working range starts at -200°C and can extend to +260°C with.. |
|||
Minimum Service Temperature, Air | -200 °C | -328 °F | |
Murtfeldt Original Material ”S”® plus + AB Polyethylene, Antibacterial Material ”S”® plus + AB contains special substances that prevent the growth of bacteria and other microbes. The material is thus ideally suited for use when manufacturing and processing foods.Sp.. |
|||
Minimum Service Temperature, Air | -200 °C | -328 °F | |
Quadrant EPP Cestidur™ Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Minimum Service Temperature, Air | -200 - -50.0 °C | -328 - -58.0 °F | Average value: -117 °C Grade Count:3 |
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi.. |
|||
Minimum Service Temperature, Air | -200 °C | -328 °F | |
GrafTech GRAFOIL® UCAR®-323 Reinforced PTFE Gasketing GRAFOIL® Grade UCAR®-323 is a laminated gasket material consisting of multiple plies of woven fiberglass coated with PTFE. It will not support combustion or bacteria. Its applications include:.. |
|||
Minimum Service Temperature, Air | -200 °C | -328 °F | |
Isoflon PTFE + 15% Graphite Polytetrafluoroethylene with 15% Graphite Properties:Good thermal conductivityLow coefficient of frictionLow permeabilityApplications: Non-lubricated dynamic seals.Information provided by Isoflon. |
|||
Minimum Service Temperature, Air | -200 °C | -328 °F | |
Guarniflon PTFE G420 Polytetrafluoroethylene 50% Steel PTFE G Special Compound with steelInformation provided by Guarniflon® |
|||
Minimum Service Temperature, Air | -200 °C | -328 °F | |
Guarniflon SC 1400 Polytetrafluoroethylene Seal SC series is a superior and unique material for gasket (flat Sealing) applications. The overall benefits of Guarniflon SC series over that of both conventional PTFE and competitive PTFE/filler blen.. |
|||
Minimum Service Temperature, Air | -200 °C | -328 °F | |
Guarniflon PTFE G415 Polytetrafluoroethylene 25% Soft Carbon PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high .. |
|||
Minimum Service Temperature, Air | -200 °C | -328 °F | |
Dalau Dalcon 021 75% Virgin PTFE, 25% Carbon Coke Applications & Industries: General: Carbon / Coke (soft) filler is good in dry running conditions, adds to the creep resistance, increases the hardness and raises the thermal conductivity of PTFE; C.. |
|||
Minimum Service Temperature, Air | -200 °C | -328 °F | |
DuPont™ Kevlar® Aramid Pulp Sold as highly fibrillated, short (0.5-1mm) fibers. Kevlar® pulps are chopped fibers that can be used as specialty additives to enhance performance by providing excellent reinforcement and viscos.. |
|||
Minimum Service Temperature, Air | -200 °C | -328 °F | |
Dalau Dalcon 001 100% Virgin PTFE Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi.. |
|||
Minimum Service Temperature, Air | -200 °C | -328 °F | |
Dalau Dalcon 021 75% Virgin PTFE, 25% Carbon Coke Applications & Industries: General: Carbon / Coke (soft) filler is good in dry running conditions, adds to the creep resistance, increases the hardness and raises the thermal conductivity of PTFE; C.. |
|||
Minimum Service Temperature, Air | -200 °C | -328 °F | |
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature.. |
|||
Minimum Service Temperature, Air | -200 °C | -328 °F | |
3M Dyneon™ ET 6210AZ Fluoroplastic Agglomerate 3M™ Dyneon™ Fluoroplastic Agglomerate ET 6210AZ is a melt processable fluoroplastic consisting mainly of alternating tetrafluoroethylene and ethylene monomer units (ETFE). This partially crystalli.. |
|||
Minimum Service Temperature, Air | -200 °C | -330 °F | |
3M Dyneon™ TF 1750 PTFE Meets ASTM D4894 Type IINon-free-flowing powder gradeVery fine particle sizeGood electrical and mechanical propertiesLow molding pressureUsed in large billet moldingExcellent for production of very .. |
|||
Minimum Service Temperature, Air | -200 °C | -330 °F | |
3M Dyneon™ TF 1645 PTFE Meets ASTM D4894 Type IV, Grade 2 resinMolding and ram extrusion powder very good free-flow propertiesGood metering propertiesGood mold filling behaviorGood electrical and mechanical propertiesUsed .. |
|||
Minimum Service Temperature, Air | -200 °C | -328 °F | |
Guarniflon PTFE G300 Polytetrafluoroethylene A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif.. |