Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Recommended |
Nye Lubricants NC-140 Grease Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Z50B Hydrogenated NBR Compound Hydrogenated Nitrile Rubber, 45-55 °IRHD. Medium acrylonitrile (ACN) content. ASTM designation = HNBR. To meet ASTM D2000 line call-out 2MDH508, A26, B16, EO16, EO36, F14, Z1, where Z1 = tensile s.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Z60B Hydrogenated NBR Compound Hydrogenated Nitrile Rubber, 55-65 °IRHD. Medium acrylonitrile (ACN) content. ASTM designation = HNBR. ASTM D2000 line call-out 2MDH614, A26, B36, EO16, EO36, F14.Applications: High strength and .. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Recommended |
Nye Lubricants 437 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Gehman T100 |
Zeon Chemicals HyTemp® 4051CG AR Polyacrylate Elastomer HyTemp 4051CG contains acrylic esters with a small percentage of a chlorine/carboxy cure site monomer. Vulcanizates have excellent oil, heat and compression set resistance.Cement grade version of Hy.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
ConocoPhillips Tacna® HD Grease NLGI Grade 1 Tacna HD is a premium quality, adhesive, extreme-pressure (EP) lithium complex grease developed for the lubrication of heavily loaded construction, mining and industrial equipment. It also is recomm.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
Dow Corning MOLYKOTE® 41 HIGH TEMPERATURE BEARING GREASE Phenyl-methyl silicone grease thickened with carbon blackInformation provided by Dow Corning |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
ChevronTexaco Delo® NLGI 1 Grease EP FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
ChevronTexaco Delo® NLGI 2 Grease EP FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | See Note 1. |
ChevronTexaco Miltex EP NLGI Grade 2 Texaco Miltex EP delivers value through:Good water resistance — Strong resistance to wash out of bearingsGood rust and corrosion protection, even in wet conditionsExtreme pressure protectionProtect.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | See Note 1. |
ChevronTexaco Molytex® EP NLGI Grade 0 Texaco Molytex EP grease delivers value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading, extending vehicle .. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
ChevronTexaco RPM® NLGI 2 Heavy Duty LC Grease EP FeaturesChevron RPM Heavy Duty LC Greases EP are multipurpose, water resistant, extreme pressure, heavy duty chassis, wheel bearing, and general purpose lubricating greases.They are manufactured usi.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | TR test, TR10 |
Daikin DAI-EL G-702 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: General purpose with excellent elongation and tear strength.Informatio.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | TR test, TR10 |
Daikin DAI-EL G-723 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Excellent mold releasability, non-sticking.Information provided by Dai.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | TR test, TR10 |
Daikin DAI-EL G-752 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | TR test, TR10 |
Daikin DAI-EL G-781 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | TR test, TR10 |
Daikin DAI-EL G-783 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Fast vulcanization, for complex shapes.Information provided by Daikin .. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | See Note 1. |
ChevronTexaco Texclad® 2 Texaco Texclad 2 delivers value through:Water tolerance — Resists washout, even when subject to gross water contamination.Excellent adhesiveness — Assures good film strength even in a wet environm.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
3M 34201 Lead Foil Tape Removable rubber adhesiveInformation provided by 3M |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
3M 4516 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
3M 4714 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Application |
3M FM01961K MC Polyester Label Products 3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Application |
3M FM0196J MC Polyester Label Products 3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Application |
3M FM05540K MC Polyester Label Products 3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Application |
3M PS470 White Yupo™ EDP Label Product 3M™ White Yupo™ EDP Label Products PS470 and PS472 are matte white opaque polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesiv.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
3M 4108 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Application |
3M 8777 Sealing Tape 3M™ Sealing Tape 8887 is a self-adhered, waterproof membrane designed for sealing on difficult to stick to surfaces. This product has a unique acrylic pressure sensitive adhesive that aggressively .. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Application |
3M FM05540K MC Polyester Label Product 3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Application |
3M PS472 White Yupo™ EDP Label Product 3M™ White Yupo™ EDP Label Products PS470 and PS472 are matte white opaque polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesiv.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Application |
3M 8067 All Weather Flashing Tape 3M™ All Weather Flashing Tape 8067 is a self-adhered, waterproof flashing membrane designed for sealing around openings and penetrations in exterior walls. This product has a unique acrylic pressur.. |