Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -17.8 °C | -0.0400 °F | Recommended |
Nye Lubricants 773A (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Alcoa KAMA 4100 Prime APET
(discontinued **) CapabilitiesGauge: .007” to .050” (178 to 1270µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Available in clear,.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Alcoa KAMA Petwich-PET 4300 Petwich-PET
(discontinued **) CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Recycled contentSi.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Alcoa KAMA 2100 Prime Clear OPS, Film
(discontinued **) CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Greene Tweed CHEMRAZ® 522 Perfluoroelastomer Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical r.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Greene Tweed CHEMRAZ® 615 Perfluoroelastomer Greene Tweed’s Chemraz® 615 exhibits outstanding high temperature properties, with a temperature range from 0°F to 615°F (-18°C to 324°C). Chemraz 615’s chemical resistance.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Greene Tweed CHEMRAZ® 618 Perfluoroelastomer Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical r.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | Approx. Cold test |
Lubriplate 3000 Moly-Lithium Type Multi-Purpose Grease Tacky, moly-lithium, extreme pressure greases that provide a durable, tenacious, adhesive film to protect against water, rust, and corrosive contaminants. 3000-W is for cold ambient temperatures.App.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | Approx. Cold test |
Lubriplate 930-AA Bentone Type Multi-Purpose Grease Formulated for higher temperature applications. They are shear stable, multi-purpose greases for both plain and anti-friction bearings. This series works well up to 375°F / 191°C and for short.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | Approx. Cold test |
Lubriplate FML 1 Anhydrous Calcium USP Mineral Oil-Based Food Machinery Grade Grease These white, multi-purpose greases have been popular in the food processing industry for years. Available in three NLGI densities for a wide variety of applications.FML Series greases are available .. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | Approx. Cold test |
Lubriplate FML 2 Anhydrous Calcium USP Mineral Oil-Based Food Machinery Grade Grease These white, multi-purpose greases have been popular in the food processing industry for years. Available in three NLGI densities for a wide variety of applications.FML Series greases are available .. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Saint-Gobain CHR® M716 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Saint-Gobain CHR® M734 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Saint-Gobain CHR® M783 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Saint-Gobain CHR® M788 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Saint-Gobain CHR® M797 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Saint-Gobain CHR® M852 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Saint-Gobain CHR® M855 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Saint-Gobain CHR® M897 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Master Bond MB600SCN Aqueous Based Electrically Conductive Sodium Silicate Coating Master Bond MB600SCN is an aqueous based, sodium silicate system with a silver coated nickel filler. It is intended for use in applications where very good shielding effectiveness is required and co.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
ConocoPhillips SUPER-STA NLGI No. 2 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Donnelly Bros APG #2 Super Clean All Purpose Mold Grease Clear, non-melting PTFE (Teflon type) extreme pressure All Purpose Grease (APG). Odorless, with a Vaseline-like texture. 100% waterproof. Mineral oil base.APG is used in the automotive, appliance,.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
ConocoPhillips EP Conolith® Grease NLGI NO. 0 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
ConocoPhillips EP Conolith® Grease NLGI NO. 00 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
ConocoPhillips Tacna® 2000 NLGI No. 1 Description: Conoco Tacna 2000 is available in two NLGI grades: No. 1 and No. 2. The No. 2 grade is ideal for use in heavily loaded sleeve-type bushings and bearings subjected to shock loading and o.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Bostik 2106 Low viscosity, quick grab EVA Glue Stick Bostik 2106 Low viscosity, quick grab EVA Glue StickLow viscosity. Quick grab for woodworking, general assembly and various plastics. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Bostik 2103 Flexible Bond EVA Glue Stick Bostik 2103 Flexible Bond EVA Glue StickFlexible bond for non-porous substrates. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Bostik 6239 Low Viscosity, High Temp Resistance, Long Open Time Polyamide Glue Stick Bostik 6239 Low Viscosity, High Temp Resistance, Long Open Time Polyamide Glue StickLow application viscosity. High temperature resistance. Long open time. Resistance to plasticizer migration for vi.. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Bostik 130 General Purpose EVA Glue Stick Bostik 130 General Purpose EVA Glue StickGeneral purpose for a variety of substrates including ABS in general assembly. |
|||
Minimum Service Temperature, Air | -17.8 °C | 0.000 °F | |
Alcoa KAMA SealPET™ 4205 RF Sealable RPET
(discontinued **) CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Silicone coating a.. |