Polymer Property : Crystallization Temperature = 252 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 116 - 122 °C
241 - 252 °F
Addcomp PRIEX® Ionomer 42101 PP homopolymer
Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t..
Crystallization Temperature 116 - 122 °C
241 - 252 °F
Addcomp PRIEX® Ionomer 40101 PP homopolymer
Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t..