Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 113 - 115 °C | 235 - 239 °F | |
Addcomp PRIEX® 20095 Maleic Anhydride Grafted PP homopolymer Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f.. |
|||
Crystallization Temperature | 113 - 115 °C | 235 - 239 °F | |
Addcomp PRIEX® 20070 Maleic Anhydride Grafted PP homopolymer Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f.. |
|||
Crystallization Temperature | 113 - 115 °C | 235 - 239 °F | ISO 11357-3 |
Addcomp PRIEX® 20097 Maleic Anhydride Grafted PP homopolymer Fields of application: Functionalised polypropylene to be used as compatibiliser for polymer blends or coupling agent for glass fibre, wood flour, natural fibres, multilayer films, aluminium foils, .. |
|||
Crystallization Temperature | 104 - 115 °C | 219 - 239 °F | Average value: 110 °C Grade Count:7 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |