Polymer Property : Crystallization Temperature = 275 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 135 - 140 °C
275 - 284 °F
Peak, DSC; ASTM D3418
Solvay Specialty Polymers Solef® 5130 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 5130 PVDF has an ultra high viscosity ideal for its usage in lithium batteries.Additional Information: Intrinsic Viscosity: 0.27 - 0.37 l/gInformation provided by Solvay Specialty Polymers.
Crystallization Temperature 135 - 140 °C
275 - 284 °F
Peak; ASTM D3418
Solvay Specialty Polymers Solef® 5130 Polyvinylidene Fluoride (PVDF)
Solef® 5130 PVDF is an ultra high viscosity grade that gives the best adhesion ideal for its usage in lithium batteries.Features: Good Adhesion; Ultra High ViscosityUses: Batteries; BinderAdditio..