Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 115.8 °C | 240.4 °F | ASTM D3418 |
LyondellBasell Alathon® M5372 High Density Polyethylene ApplicationsALATHON M 5372 copolymer with narrow weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing stability. .. |