Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 95.0 - 104 °C | 203 - 219 °F | Average value: 98.4 °C Grade Count:10 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |