Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Crystallization Temperature = 261 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 261 °C
502 °F
ISO 3146
ExxonMobil PP4031E2 Polypropylene Impact Copolymer
Product Description: An impact copolymer resin for extrusion applications with high melt viscosity and excellent rigidity, shock resistance and dimensional stability. It is designed for corrugated ..
Crystallization Temperature 261 °C
502 °F
ISO 3146
ExxonMobil PP7064L1 Polypropylene Impact Copolymer
Product Description: A nucleated impact copolymer resin with medium flow, high stiffness and antistatic properties. It is suitable for molding applications like consumer products, closures, contain..